Recent studies on the solubility of Equation or symbol description not availableGd2O3 in Equation or symbol description not availableCeO2 and high-temperature aging behavior of solid solutions Equation or symbol description not availableCe1−xGdxO2−δ Equation or symbol description not available(0.05⩽x⩽0.4) are presented. X-ray diffraction analysis indicated that 1600°C sintering was sufficient to ensure the dissolution of Equation or symbol description not availableGd2O3 into Equation or symbol description not availableCeO2 to form solid solutions. High-temperature aging at 1000°C showed a significant effect on the electrical conductivities of the Equation or symbol description not availableCe1−xGdxO2−δ ceramics. For the compositions Equation or symbol description not availablex<0.2, high-temperature aging led to an increase in the total conductivity resulting mainly from an improved grain boundary behavior. However, for the compositions Equation or symbol description not availablex>0.2, high-temperature aging had a detrimental effect on both the grain interior and grain boundary conductivities. The grain interior and grain boundary conductivities of the Equation or symbol description not availableCe0.75Gd0.25O2−δ ceramic were reduced by 30 and 44%, respectively, as a result of high-temperature aging at 1000°C for 8 days. The aging behavior of doped ceria cannot be explained using the mechanisms applied to doped zirconia. © 2004 The Electrochemical Society. All rights reserved.