Zirconium silicate Equation or symbol description not available[(ZrO2)X(SiO2)1−X] films were deposited by using a combination of precursors: tetrakis(diethylamido)zirconium Equation or symbol description not available[Zr(NEt2)4] and Equation or symbol description not availabletetra­n­butyl orthosilicate Equation or symbol description not available[Si(OnBu)4]. An atomically flat interface of silicate/silicon was observed with no interfacial silicon oxide layers and impurity concentrations were less than 0.1 atom % (below detection limits). Zirconium silicate films with Equation or symbol description not available∼20% Equation or symbol description not availableZrO2 were amorphous up to 800°C and, above 900°C, phase separation of the films occurred into crystal Equation or symbol description not availableZrO2 and amorphous phases. Dielectric constant Equation or symbol description not available(k) of the Zr-silicate films was about 7.3. Hysteresis in capacitance-voltage Equation or symbol description not available(C­V) measurements was less than 0.02 V. The leakage current density was Equation or symbol description not available1.63×10−4A/cm2 at a bias of 1.0 V. © 2004 The Electrochemical Society.