Equation or symbol description not available(Ba1−xSrx)TiO3 (BST) films were deposited on the new electrode structures of Equation or symbol description not availablePt/RuO2+Ta/TiSi2/poly‐Si/SiO2/Si (PRTS) and Equation or symbol description not availablePt/RuO2+Ta/poly‐Si/SiO2/Si (PRS) by metallorganic chemical vapor deposition. The films deposited on PRTS show smoother morphologies than those on PRS. Titanium‐silicide Equation or symbol description not available(TiSi2) buffer layers formed on poly‐Si play an important role in decreasing the roughness of each layer as well as contact resistance between Equation or symbol description not availableRuO2+Ta and poly‐Si. The electrode structures showed a stable morphology after deposition of BST films and annealing at 750°C. The 80 nm thick BST films deposited on PRTS showed a dielectric constant of 240 and dissipation factor of 0.01 at 100 kHz. The BST films deposited on PRTS have a leakage current density of about Equation or symbol description not available4.0×10−7A/cm2 at 190 kV/cm and breakdown strength of 290 kV/cm. © 1999 The Electrochemical Society. All rights reserved.