Metastable scheelite Equation or symbol description not availableEuVO4 was stabilized by a high temperature and pressure method, which was transformed into a stable zircon phase by annealing treatment in air. Scheelite Equation or symbol description not availableEuVO4 gave strong emissions with a dominant peak at 617 nm associated with the Equation or symbol description not available5D0­7F2 transition of Equation or symbol description not availableEu3+. Equation or symbol description not available151Eu Mössbauer spectra indicated that the isomer shift for the metastable scheelite phase was ca. 0.5 mm/s lower than that for the zircon phase, which was ascribed to a reduced covalency in the Eu-O bond originated via a charge transfer from oxygen to Equation or symbol description not availableEu3+ in scheelite lattice by producing an enhanced shielding of 4f electrons on the s orbital as well as a decrease in s electron density around Equation or symbol description not availableEu3+ nucleus. Impedance spectra for the zircon phase clearly demonstrated an ionic hopping in the bulk with a conductivity of ca. Equation or symbol description not available1.0×10−3 S cm−1 at 500°C. Equation or symbol description not availableEuVO4 is proved to be both a potential phosphor and a potential ionic conductor. © 2001 The Electrochemical Society. All rights reserved.