Errata
2078
The following article is Free article
Shigemi Kohiki, Sei Fukushima, Hideki Yoshikawa and Masao Arai
1667
Takemi Ueki, Manabu Itsumi and Tadao Takeda
We analyzed the side-wall structure of grown-in octahedral defects in Czochralski silicon standard wafers for large-scale integrated circuits. There are two types of twin octahedral defects: an overlapping type and an adjacent type. In the twin octahedral defects of the overlapping type, a hole is formed in the connection part. The side-wall layer in the hole part is formed continually and is the same thickness as the side-wall layers of both octahedrons. In the twin octahedral defects of the adjacent type, a partition layer is formed in the connection part. Our electron energy-loss spectroscopy analyses identified that the side-wall layer includes SiO2.
1671
Wai Kin Chim and Gim Leong Teh
Neutral electron trap generation and hole trapping under electrostatic discharge (ESD) stressing of thin oxides are investigated. The results show that the number of neutral electron traps generated by the ESD stress has an empirical power-law relation to the charge injected during ESD stress. Hole trapping is also shown to be linearly related to neutral electron trap generation, the slope of the straight line in a plot of the two quantities against each other being close to unity. This suggests that the hole traps and neutral electron traps originate from the same mechanism under ESD stress.
1674
Jiro Ida and Atsushi Ohtomo
The TiSi2 local wiring technology has been newly characterized from the viewpoints of dopant interdiffusion and power reduction. It was found that only the p+/n junction degrades when TiSi2 local wiring connects the n+ layer and p+ layer. The results of electrical measurements using a set of new test patterns suggest the reason to be that boron does not diffuse from TiSi2 to Si due to the high efficiency of TiB formation. More than a 20% reduction in power dissipation at a low-power supply voltage of 1 V was obtained, which demonstrates that the scheme is promising for low-power sub-half-micron complementary metal oxide semiconductor.
1680
Atsushi Ando, Kunihiro Sakamoto, Kazushi Miki, Kazuhiko Matsumoto and Tsunenori Sakamoto
We have demonstrated the characterizations of the morphologies and local electrical properties of the SiO2/Si(001) structure which was formed by oxidation of the spatially controlled atomic-step-free Si(001) surface. The two-dimensional current images and current-voltage characteristics showed spatial differences in the local electrical properties while the morphologies at the SiO2 surface and the interface between SiO2 and Si(001) were uniform, with root-mean-square values of roughness, smaller than a monoatomic-step-height.
1684
Kazutoshi Shiba, Seiichi Miyazaki and Masataka Hirose
The temperature dependence and the temporal decay of photoluminescence from thermally-oxidized porous silicon have been studied under 1.80 or 2.54 eV excitation which is below or above the optical bandgap value of 2.2 eV determined from the luminescence excitation spectrum. No significant difference between luminescence spectra under the subgap and the overgap excitation is observed at emission energies below 1.65 eV. The luminescence under the subgap excitation exhibits a weak temperature dependence compared to the overgap excitation case. This can be interpreted in terms of the suppressed thermal emission-rate for carriers photogenerated near the radiative recombination centers to the extended states. It is also revealed that, in the pulsed subgap excitation, the luminescence shows a fast decay in the time region below 1 µs and a slow decay component follows, as observed in the case of the pulsed overgap excitation. The carriers photogenerated directly at radiative recombination centers or neighboring sites under the subgap excitation are likely to be responsible for the observed fast decay.
1689
Hideki Takahashi, Hiroshi Yamada-Kaneta and Masashi Suezawa
The gettering efficiency of iron (Fe) was investigated as a function of the size and density of oxygen precipitates in Czochralski-grown silicon (CZ-Si). During the precipitation treatments, in order to control the size and density of oxygen precipitates, we monitored the oxygen concentration ([Oi]) so that the final [Oi] of the samples were equal to each other. By comparing Fe concentration ([Fe]) determined by electron spin resonance (ESR) in the samples, we discovered that the sample containing precipitates of large size and low density has a stronger gettering efficiency during cooling from a temperature of 1050°C. In contrast, the sample containing precipitates of small size and high density has a stronger gettering efficiency during isothermal annealing at 190°C.
1693
Masashi Uematsu
Sb diffusion profiles in heavily As-doped Si have been simulated using just two essential parameters for Sb diffusion. These parameters correspond to the diffusion of dopant species that contribute to Sb diffusion, and they are the effective diffusivities of the vacancy mechanism via single and double negatively charged vacancies. We discuss which diffusing species affect diffusion profiles based on the integrated diffusion model.
1697
Akio Itoh, Masahiko Imai and Yoshihiro Arimoto
We investigated the chemical mechanical polishing (CMP) characteristics of photoresist for the first time. It was found that photoresist polishing rates are strongly dependent on photoresist baking temperature. The photoresist polishing rate exceeded 7000 nm/min, which is 87 times higher than the value for SiO2, after baking at 170°C, but matched that of SiO2 after baking at 220°C at a polishing pressure of 230 g/cm2. The photoresist polishing rate after baking at 240°C was lower than that of SiO2. Using these photoresist CMP characteristics, a simple shallow trench isolation (STI) process was achieved.
1701
Chang-Sik Son K. Park, Seong-Il Kim Kyu Kim, Suk-Ki Min Suk-Ki Min and In-Hoon Choi In-Hoon Choi
Maskless one-step selective CCl4-doped GaAs epilayers have been grown on patterned GaAs substrates by atmospheric pressure metalorganic chemical vapor deposition. The growth technique has potential for realizing a well-defined quantum confinement structure and lateral structure device. Round shaped CCl4-doped GaAs epilayer was selectively grown inside a U-groove and on the sidewalls of a mesa with a significant lateral growth rate enhancement, whereas no growth was observed outside U-groove and on top of the mesa.
1704
G. Y. Zhao, Hiroshi Ebisu, Tetsuo Soga, Takashi Egawa, Takashi Jimbo and Masayoshi Umeno
The electrical transport property of GaSb are analyzed, both experimentally and theoretically. It is demonstrated that the mobility of GaSb is limited not only by high unintentionally doped impurity concentration, but also by high compensation ratio. Hall-effect measurement are made between 300 and 20 K on several undoped GaSb samples. It is found that the electrical properties of GaSb epilayers strong depend on growth temperature, and the impurity conductivity dominated the conduction mechanism over a large temperature range.
1709
Masahiro Yoshimoto Masahiro Yoshimoto, Yasuhiro Watanabe Yasuhiro Watanabe and Hiroyuki Matsunami Hiroyuki Matsunami
GaAs1-xPx (0.2<x<0.7) was grown on a Si substrate with a GaP buffer layer by metalorganic molecular beam epitaxy. The surface smoothness was taken to be an indicator for the improvement of GaAsP crystallinity. The optimal growth temperature and thickness of the buffer layer for obtaining a smooth surface were determined based on results of atomic force microscopy and reflection high-energy electron diffraction. While GaAsP epilayers grown directly on Si showed no photoluminescence (PL), GaAsP grown on Si with a thin GaP buffer layer (∼100 Å) at 300°C showed PL. GaAsP epilayers of n-type were obtained with Sn-doping during growth. The electron conduction in n-type GaAsP was explained by carrier conduction in both the Γ valley and the X valley.
1715
Gunther Vollrath, Andreas Schlachetzki and Friedrich Fiedler
In this paper ion-beam-milling of GaAs, InP as well as of InGaAs and InGaAsP of different compositions lattice-matched to InP was investigated using nitrogen and nitrogen/oxygen mixtures. The influence of process parameters such as gas composition, kinetic energy of the ions and the angle of incidence of the ions was investigated in detail. The etch rates of different masking materials like titanium, photoresist and SiO2 are also given. Special attention was paid to the geometry and roughness of the mesa facets in view of their use as laser facets. For the first time the experimental results are compared to calculations based on the sputter theory of Sigmund. The calculated dependence of the etch rates on the kinetic energy of the ions and on the angle of incidence up to 40° is in good agreement with the experimental results.
1721
G. A. Armstrong, S. Uppal, S. D. Brotherton and J. R. Ayres
A new physical model based on two dimensional simulations for high quality laser re-crystallised poly-Si thin film transistors is presented. It has been shown that to adequately explain the improved subthreshold slope and the lack of saturation of the output characteristics in these transistors, it is essential to distribute the density of defect states between traps in the grains alongside traps localised at grain boundaries. A double exponential density of states has been extracted for thin film transistors (TFTs) annealed at different excimer laser energies, using the field effect conductance method. By splitting the density of states between grain traps and grain boundary traps good fits to the output characteristics have been achieved. Lack of saturation is shown to be due to decrease in potential barrier at grain boundaries with increase in drain bias. At high gate voltages, however, evidence of a self-heating effect similar to that observed in silicon-on-insulator (SOI) transistors is apparent.
1727
Kwon-Young Choi, Kee-Chan Park, Hyoung-Bae Choi and Min-Koo Han
We have proposed and fabricated a new bottom-gate poly-Si thin-film transistor (TFT) with local amorphous-Si region in the channel by employing the selective laser annealing. The ON/OFF current ratio of the new poly-Si TFT is larger by the magnitude of three orders than that of conventional poly-Si TFT. In the proposed device, the significant reduction of leakage current may be obtained due to the highly resistive a-Si region. However, under the ON state, the resistance of local a-Si is decreased significantly by the inducement of channel electrons in the a-Si channel. The total mask number and the fabrication process of the proposed device are almost identical to those of a commercial a-Si:H TFT.
1730
Frank Siebke Frank Siebke, Shigeo Yata Shigeo Yata, Yoshihiro Hishikawa Yoshihiro Hishikawa and Makoto Tanaka Makoto Tanaka
Undoped microcrystalline silicon with various crystallinities was deposited by rf-glow discharge. We investigate the correlation between crystallinity and optoelectronic properties. The use of a constant photocurrent method for characterization of undoped microcrystalline silicon is discussed. In the case of high crystallinity this method measures the true absorption coefficient but with decreasing crystallinity, the constant photocurrent method underestimates the absorption coefficient at low photon energies. At these energies, carriers are mainly photo generated in the crystalline phase. Carriers generated in isolated grains give a smaller contribution to the photocurrent than carriers generated in grains forming percolation paths. This results in a strongly decreased absorption coefficient measured by the constant photocurrent method at photon energies of about 1.7 eV and below. Therefore, stable microcrystalline silicon with a high crystallinity can be easily distinguished from an unstable material with poor crystallinity.
1736
Rosa Chierchia Rosa Chierchia, Stefano Loreti Stefano Loreti, Vittorio Loreto Vittorio Loreto, Luigi Mariucci Luigi Mariucci, Carla Minarini Carla Minarini and Alberto Mittiga Alberto Mittiga
We have studied the light degradation and the thermal annealing of a-Si:H at different light intensities and temperatures monitoring both the defect density and the photoconductivity. This large set of data is used as a benchmark for the models of the metastability in a-Si:H. We show that an entire class of these models (which predict stretched exponential kinetics) is not in good agreement with our data. We discuss the mathematical and physical basis of these models pointing out some weak points that could explain these failures. The data are in better agreement with the “recombination induced bond breaking" models if an accurate description of annealing processes is included. The annealing rate must be computed considering a broad distribution of energy barriers. It must be also taken into account that the energy barrier for the annealing of a metastable defect can be reduced by a monomolecular trapping event at the defect itself. Our calculations show that this reduction amounts to an energy of about half the gap and lasts for a time of the order of 1 ps.
1747
Keiji Tanaka
The first sharp diffraction peak which signifies medium-range structural order in chalcogenide glasses has been studied based on some observations and the construction of ball-and-stick models. The crystalline model originally proposed by Vaipolin and Porai-Koshits provides straighforward explanations for most features.
1754
Minoru Kumeda Minoru Kumeda, Akio Masuda Akio Masuda and Tatsuo Shimizu Tatsuo Shimizu
ESR signals for hydrogenated amorphous Ge–C alloy films prepared by magnetron sputtering were deconvoluted into signals originating from a Ge dangling bond and a C dangling bond. It was determined from the results of the deconvolution that the number of Ge dangling bonds per Ge atom is ten to sixty times larger than that of C dangling bonds per C atom. In contrast to the case of Ge–Si alloy films, in which the number of Ge dangling bonds per Ge atom decreases by increasing the Si content because of the increase in the density of Si–H bonds, the number of Ge dangling bonds per Ge atom increases by increasing the C content in Ge–C alloy films, although the density of C–H bonds increases. This finding may be caused by an increase in the structural randomness because the difference in the covalent bond radius between Ge and C is quite large.
1760
Hiroyuki Sano, Hiroshi Hirasawa, Susumu Nakamura, Kenichi Kondo and Katsuaki Sato
CuIn(SxSe1-x)2 thin films were prepared on Mo-coated soda-lime glass substrates by the ionized cluster beam (ICB) technique, in which Cu, In2S3 and Se vapors were ionized and accelerated. The substrate temperature was kept at Ts=400°C. The films were characterized using X-ray diffraction (XRD), a scanning electron microscope (SEM), and an electron-probe microanalyzer (EPMA). It was found that polycrystalline films with improved grain size were obtained when the substrate temperature exceeded 250°C. Using the ICB technique, thin film solar cell devices based on these CuIn(SxSe1-x)2 films were fabricated. The photovoltaic effect was confirmed in substrate-type structure solar cells with the low-temperature deposition of ICB-grown CuIn(SxSe1-x)2 thin films.
1764
Shui Hsiang Su, Meiso Yokoyama and Yan Kuin Su
ZnS epitaxial layers grown using metalorganic vapor phase epitaxy were etched by reactive ion etching (RIE) employing a gas mixture of CH4, H2 and Ar. The etching rates were investigated as functions of the plasma parameters: rf power density, the relative composition and the total flow rate of reactive gases. It was determined that the amount of CH4 in CH4/H2 gas discharge decides whether a polymer will be produced. The optimum composition of the mixed gas was 1CH4/7H2/4Ar, when the pressure, rf power density and total flow rate were 30 mTorr, 0.4 W/cm2 and 30 sccm, respectively. The quality of the etched surfaces under these conditions was examined using X-ray photoelectron spectroscopy and photoluminescence. It was determined that the etching process does not damage the ZnS film based upon the results of photoluminescence spectra.
1768
Doo-Hyeb Youn, Maosheng Hao, Hisao Sato, Tomoya Sugahara, Yoshiki Naoi and Shiro Sakai
Investigations of the new metal scheme for ohmic contact to p-GaN have been carried out. The specific contact resistance was measured to be ρc=3.6×10-3 Ω cm2 which is the lowest value ever reported for moderately doped p-GaN (4.4×1017/cm3). All metals were deposited on metalorganic chemical vapour deposition (MOCVD) grown p-GaN. The interaction mechanism between Ni and p-GaN has been investigated. Zn diffusion has been observed during annealing in Au–Zn/Ni on p-GaN. The interfacial reaction mechanism during annealing has been studied by secondary ion mass spectroscopy (SIMS) measurement. From this measurement, it is observed that Ni dissociates at the p-GaN surface and this dissociation promotes the Zn diffusion upon heat treatment. The electrical properties were studied using current–voltage (I–V) measurements at room temperature. The microstructure between the Ni and p-GaN interface was investigated using high-resolution transmission electron microscopy (TEM) before and after the heat treatment.
1772
Sheng-Lyang Jang, Chwan-Gwo Chyau, Shau-Shen Liu and Chung-Ming Chiu
In this paper, we report a complete, single-piece, and analytical drain current model for submicrometer buried-channel (BC) lightly-doped drain (LDD) metal oxide semiconductor field effect transistors (MOSFETs). The model is valid in all regions of operation, is suitable for a circuit simulator, and is developed using the quasi-two-dimensional approach. The BC device physics, bias-dependent LDD resistance, velocity saturation, drain induced barrier lowering and channel length modulation have been taken into account in the model. The accuracy of the resulting LDD BC MOSFET model has been checked by the experimental LDD data.
1781
Alain Chantre, Thierry Gravier, Stéphan Niel, Jean Kirtsch, André Granier, André Grouillet, Marc Guillermet, Delphine Maury, Roland Pantel, Jorge Luis Regolini et al
Two innovative process technologies are introduced to overcome problems related to the downscaling of single-polysilicon self-aligned bipolar transistors. First, the use of a selective silicon deposition step before Ti salicidation of the structure is shown to improve TiSi2 formation on narrow As-doped polysilicon emitters. At the same time, the elevation of the extrinsic base regions around the emitter causes a significant reduction of peripheral electron recombination effects. Second, the implantation of the intrinsic base at a large tilt angle (LATIB) is demonstrated to suppress emitter-to-collector punchthrough along the isolation edges. The first 0.35 µm single-polysilicon self-aligned bipolar transistors fabricated using a 200 mm complementary metal oxide semiconductor (CMOS) derived bipolar process integrating these novel process technologies are described.
1787
Doo-Young Kim, Seong-Dong Kim, Min-Koo Han and Yearn-Ik Choi
A hybrid-mode operation of silicon-on-insulator (SOI) bipolar mode field effect transistor (BMFET) is proposed to improve the current gain. The device characteristics are analyzed and verified numerically for hybrid mode, BMFET mode, and double-diffused metal-oxide-semiconductor field effect transistor (DMOS) mode by MEDICI simulation. In hybrid-mode operation, DMOS, lateral bipolar transistor, and BMFET currents flow simultaneously. The proposed SOI BMFET exhibits 30 times larger current gain in hybrid mode operation by connecting DMOS gate to the p+ gate of BMFET structure as compared with the conventional structure without sacrifice of breakdown voltage and leakage current characteristics. The improved current gain characteristics are achieved by the DMOS-gate-induced hybrid effect that lowers the barrier of p-body and reduces the charge in the p-body.
1793
Risho Koh Risho Koh
A body-driven silicon-on-insulator metal-oxide-silicon field-effect-transistor (body-driven SOI-MOSFET, BD-MOS) is proposed, and the device characteristics are estimated using a device simulator. This device can remove excess holes within several picoseconds. Additional body contact, which requires additional device area, is not required for removing holes. A small S factor (76 mV/dec.) and a small Vth roll-off (ΔVth=15 mV for ΔVd = 0.4 V) were obtained for the channel length of 0.08 µm, without using very thin gate oxide. An enhancement operation and the large drain current required for complementary-MOS(CMOS)-compatible circuits are achieved.
1801
J. Richard Ayres, Stan D. Brotherton, David J. McCulloch and Michael J. Trainor
Hot carrier instabilities in poly-Si thin film transistors (TFTs) are caused by high electric fields at the drain. These high fields are determined mainly by the abruptness of the lateral n+ doping profile in the drain and the two-dimensional (2D) coupling of the x and y components of the electric field between the gate and drain. The density of trapping states in the poly-Si film, however, has a much less significant impact on the field. Further, it is shown that improving the properties of the poly-Si film tends to have an adverse affect on hot carrier stability. Consequently, it is concluded that drain field relief is essential for hot carrier stability of n-channel poly-Si TFTs. It is shown that gate overlapped lightly doped drain (GOLDD) architectures can be used to relieve the drain field without introducing series resistance. Stable TFTs have been fabricated with GOLDD, consistent with circuit operation up to drain biases of 20 V. GOLDD is also effective in reducing the field enhanced leakage current in the off-state.
1809
Kazuhiko Endo, Toru Tatsumi, Yoshihisa Matsubara and Tadahiko Horiuchi
Fluorinated amorphous carbon thin films (a-C:F) for use as low-dielectric-constant interlayer dielectrics are deposited by helicon-wave plasma-enhanced chemical vapor deposition using fluorocarbon compounds as a source material. The a-C:F films can be grown from C4F8 at a high deposition rate (above 400 nm/min) and they are thermally stable up to 350°C. The addition of bias power to the substrate makes it possible to completely fill gaps in the wiring (space 0.35 µm, height 0.65 µm) with the a-C:F film. To protect the a-C:F film during further processing, a SiO2 film is deposited to add mechanical strength and resistance to the oxygen plasma used to remove resist materials. The adhesion between the a-C:F and SiO2 films is dramatically improved by inserting an adhesion promoter consisting of a-C:H and Si-rich SiO2. By using the a-C:F and SiO2 dielectrics and chemical mechanical polishing (CMP) process, globally planarized 3-level metallization is achieved. The a-C:F dielectric can reduce inter-line capacitance close to a half value as compared with the conventional SiO2 dielectrics.
1815
Yutaka Tokuda
Hydrogen has been introduced into 10 MeV electron-irradiated n-type silicon by wet chemical etching. The introduction of hydrogen causes the reduction of the concentration of the A center and divacancy, while it induces the formation of the NH1 electron trap (Ec-0.31 eV). The NH1 trap is found to correspond to one of the hydrogen-related traps in hydrogen-implanted n-type silicon, which has not been observed in electron-irradiated hydrogenated n-type silicon. The NH1 trap is tentatively ascribed to the vacancy-oxygen pair which is partly saturated with hydrogen.
1817
Tadao Toda, Yasuhiro Ueda and Akira Ibaraki
A 6H-SiC Au-gate metal-semiconductor field-effect transistor (MESFET) was fabricated by reactive ion etching (RIE) for device isolation and ion implantation for the n+ contact regions of the source and drain. The device exhibited a pinch-off voltage of -9 V, transconductance (gm) of 5.3 mS/mm, and gate breakdown voltage of -200 V. The characteristics of the MESFET were investigated at high temperatures. This MESFET can be operated at 400°C.
1819
Ming-Sheng Leu, I-Chung Tung and Tsung-Shune Chin
The crystallization fraction (Xf) was quantitatively determined by the decrement in the crystallization enthalpy of an annealed Fe78Si13B9 alloy as compared with that of the as-cast one. The Xf was used to interpret the variation in ac-initial permeability (µi) of the Fe78Si13B9 alloy in-situ measured during isothermal annealing at 646 and 666 K, respectively. There are two µi maxima as soaking time elapses for both annealings. The first µi maximum is attributed mainly to the stress-relaxation effect and some crystallization effect with a measured Xf of 2–3.5%. The second µi maximum, appearing at about 210 and 36 ks for the annealings at 646 and 666 K, respectively, is invariantly much higher than that of the first one. The two corresponding crystallization fractions (Xf) are the same, about 9 % for both annealings. The second maximum is thus associated with crystallization effect. The Curie temperature of the amorphous matrix, being 668.5 K for the as-cast sample, increases sharply with annealing time. This makes difference in the shape of the first maximum, leveling off for the 646 K annealing and sharpening for the other. Transmission electron microscopy (TEM) micrographs and X-ray diffractometry (XRD) studies of the crystallized α-Fe and Fe(Si) phases in the alloy annealed at 646 K for more than 180 ks were depicted.
1825
Fumio Maruyama, Hiroyuki Nagai, Yasushi Amako, Hiroshi Yoshie and Kengo Adachi
In order to study the magnetic properties of the Co-sublattice of R2Co7B3, the 59Co NMR and magnetic measurements have been carried out at 4.2 K. The R2Co7B3 (R=Y, Ce, Nd, Sm and Gd) compounds with a hexagonal Ce2Co7B3-type structure are obtained. The Co moments at the 6i1 site are estimated from NMR and are found to be nearly consistent with those obtained from the magnetic measurements for R=Y, Sm and Gd. On comparing the calculated moments per unit cell, µ, with the saturation magnetization, Ms, for R=Y and Gd, the values of µ are found to be very consistent with those of Ms and the value of µ for R=Ce is much larger than that of Ms.
1829
Lihong Li Lihong Li, Ken'ichiro Yashiro Ken'ichiro Yashiro and Sumio Ohkawa Sumio Ohkawa
Numerical analysis of the attenuation of magnetostatic wave envelope (MSWE) solitons has been performed to obtain a good insight into the decay properties of MSWE solitons. The numerical calculations indicate that the amplitude of MSWE wave-packets decays at the rate of exp
(- αηt) in yttrium iron garnet films, where α is an attenuation factor and η is a damping coefficient. The value of α is found to be dependent on the ratios of dispersion to dissipation and nonlinearity to dissipation and to vary in the range of 1 ≤α≤2 . The full-width at half maximum of MSWE solitons broadens due to loss and the broadening rate is as sensitive to loss as the amplitude decay rate. The decay characteristics of MSWE solitons presented here provide us with useful information on how to choose experimental parameters for the formation of MSWE solitons.
1833
Fumiko O. Shimizu, Takahiro Homma, Masaya Nakao, Hiroki Takahashi, Tadashi Hirata and Arimichi Minoh
From the peak output power measurement for the optically pumped CO2 4.3 µm pulse laser, the effect of foreign gas and the molecular dynamics are examined. For the CO2 4.3 µm and 10.6 µm pump sequence laser pulses occurring in the same discharge tube, the optimization of the peak output power is discussed. The J-profile of delay time from the start of the pump sequence pulse to the peak of the 4.3 µm laser pulse indicates that rotational relaxation due to CO2–CO2 collision via |ΔJ|=2 transition occurs, and also suggests the inclusion of the |ΔJ|>2 transition process.
1838
Takuya Murata, Akira Fujimoto, Toshikatsu Miki and Shin'ichi Sakata
The optically nonlinear Li3VO4 crystal grown by the floating-zone (FZ) method has been characterized by optical absorption and electron spin resonance (ESR) spectroscopy. The as-grown single crystals grown in gaseous argon exhibit a broad absorption extending from the uv to near-infrared light regions and an absorption band at about 3 eV. Postoxidation reduces the whole optical absorption and reveals an additional 1.9 eV band. ESR detects several signals associated with transition-metal ions in as-grown and reduced crystals, i.e., Fe3+, Mn2+ and Cr3+ ions. The Mn2+ and Cr3+ signals are absent in well-oxidized crystals, while the Fe3+ signal shows no significant change. The reduced crystals have three absorption bands associated with transition-metal impurities and oxygen vacancies. The diffuse reflectance spectra of transition-metal-doped Li3VO4 polycrystals were also measured to examine the effect of the presence of Fe3+, Mn2+ and Cr3+. The origin of the optical absorption in as-grown, oxidized and reduced Li3VO4 are discussed in terms of unexpectedly doped iron-group transition-metals and oxygen vacancies. The 3 eV and 1.9 eV absorption bands and the broad band extending from the uv to near-infrared regions are suppressed in the well-oxidized crystals subjected to repeated zone refining, indicating that multiple zone refining and complete oxidation are important in obtaining optical-quality Li3VO4 single crystals.
1842
Gaoyang Zhao, Noboru Tohge and Junji Nishii
A new process for the fabrication of diffraction gratings has been proposed using photosensitive Al2O3 gel films in combination with a phase mask. Photosensitive Al2O3 gel films were derived from Al(O-sec-Bu)3 chemically modified with benzoylacetone. These gel films exhibited an optical absorption band in the UV-range, which is associated with the π–π* transition of chelate rings of the β-diketonate ligand. The irradiation of these gel films with XeF and KrF excimer lasers decreased their solubility in acetone containing 1.2 vol%HNO3, simultaneously with the dissociation of the remaining chelate rings. The above findings were applied to the fabrication of Al2O3 film diffraction gratings on Si and silica substrates; the gel films were irradiated with the excimer lasers through a phase mask, leached, and then heat-treated. The diffraction efficiency of the fabricated gratings was evaluated in reflection (Si sub.) and transmission (silica sub.) modes with respect to the preparation conditions.
1847
Kusato Hirota and Gentaro Ohbayashi
Phase change optical recording disks using a Pd–Ge–Sb–Te quaternary alloy demonstrated high crystallization speed and long-term thermal stability of the amorphous recording marks. This alloy film can be crystallized by a short duration laser pulse of less than 100 ns. It is applicable to a single beam overwrite optical recording system. The crystallized portion of this recording layer on the disk is assigned to single phase and polycrystalline face-centered-cubic (fcc) crystals by transmission electron diffraction. A small amount of Pd atoms (typically 0.2 to 3 at.%) in this alloy improve the thermal stability of amorphous marks.
1852
Junji Tominaga, Takashi Nakano and Nobufumi Atoda
Crystallization mechanism of Ge2Sb2Te5 thin films sandwiched between SiN layers was optically investigated and double transition temperatures were observed in the case of Ge2Sb2Te5 film thickness of more than 20 nm. The activation energies were estimated by both Kissinger's and Johnson-Mehl-Avrami equations, and it was found that the reaction order was 2 for the first crystallization and 1 for the second transition. The lower transition temperature was strongly affected by the top SiN film thickness, and it was suggested that crystallization occurred at the interface between the recording film and the top SiN layer. The second crystallization occurred at the interface between the bottom SiN and the recording layers, which was not greatly affected by the thicknesses of both films.
1855
Bekir S. Yilbas, M. Sami and K. Danisman
Laser successive pulse heating of engineering surfaces becomes fruitful for thermal treatment of the engineering parts. In this case, thermal integration of the surface temperature becomes essential. In the present study, a 3-dimensional mathematical model allowing a laser successive pulse heating is introduced using an electron kinetic theory approach. A laser beam is considered to scan the workpiece surface with a constant velocity. However, the energy equation so derived is in the form of an integro-differential equation which does not yield an analytical solution. Therefore, a numerical method using an explicit scheme is introduced to obtain the temperature profiles. It is found that energy gain of the lattice site atoms through successive electron-phonon collisions is considerable in the surface vicinity. Moreover, some oscillations in surface temperature occur in response to repetitive pulse frequency. It is less likely that the temperature profile follows the pulse profile which is due to the conduction losses and the motion of the slab.
1865
Taiju Takahashi Taiju Takahashi, Shigeru Hashidate Shigeru Hashidate, Hirokazu Nishijou Hirokazu Nishijou, Makio Usui Makio Usui, Munehiro Kimura Munehiro Kimura and Tadashi Akahane Tadashi Akahane
A new measurement method for the flexoelectric coefficients e11 and e33 (corresponding to the splay and bend strain, respectively) of nematic liquid crystals (LCs) is proposed. The values of e11+e33 and e11-e33 can be determined by fitting experimental electrooptical characteristics of hybrid aligned nematic (HAN) cells with numerical simulations. For the measurement of e11+e33 and e11-e33, a dc electric field is applied along the cell normal and along the cell surface, respectively. The measurements were carried out for two nematics, N-(4-methoxybenzylidene)-4′-n-butylaniline (MBBA) and ZLI-4792. As a result, e11+e33=(-5.4 ±1.0) ×10-11 C/m and e11-e33=(1.4 ±0.1) ×10-11 C/m for MBBA, | e11+e33 | ≤1.0 ×10-11 C/m and e11-e33=(-1.5 ±0.1) ×10-11 C/m for ZLI-4792 were obtained.
1870
Pung Keun Song, Yuzo Shigesato, Itaru Yasui, Cleva W. Ow-Yang and David C. Paine
Tin-doped indium oxide (ITO) films were deposited by dc magnetron sputtering using oxide (ITO) or alloy (IT) targets. The ITO films sputter-deposited using Ar at total pressure (Ptot) lower than 1.2 Pa showed polycrystalline structure, whereas entirely amorphous films were deposited at Ptot higher than 1.4 Pa, indicating that the crystallinity of the ITO films were heavily affected by Ptot. This was quantitatively explained in terms of the kinetic energy of sputtered particles reaching to the substrate surface, which decreased due to an increase in collision frequency between the sputtered particles and sputtering gas molecules. ITO films were also deposited using Xe or He as sputtering gases, where amorphous films were deposited at Ptot higher than 0.7 Pa (Xe) and 12 Pa (He), respectively. Based on a hard sphere collision model, the energy loss rates of the sputtered particles due to collision with sputtering gas molecules were estimated to be consistent with the experimental results for the case of using He, Ar or Xe gases.
1877
Hyun-Seo Oh, Hyung-Wook Jeon, Sergey A. Shestak, Sung-Kyu Kim, Jung-Young Son, Hyuk-Soo Lee, Yong-Jin Choi and Chang-Eon Kang
A holographic video system operated by a pulse laser is described. The use of a pulse laser as the light source allows the polygon mirror (or scanners) in the system to be eliminated. At the same time, a single long aperture acousto-optic modulator (AOM) is replaced by 6 small aperture AOMs linearly aligned and a still polygon mirror set is used. The effective aperture length of the 6-AOM-combination is 6 times that of an individual AOM. Since in this system the computer-generated-hologram (CGH) data is divided into 6 equal parts and loaded into the corresponding AOMs independently and synchronously, the loading time of CGH data to an AOM is reduced. This system can display 36,864 (in the horizontal direction)×128 (in the vertical direction) holographic fringe data points in binary format and operate at a rate of 60 frames per second using a personal computer.
1882
Kunio Yoshida Kuzuu
The laser-induced damage threshold (LIDT) of various types of silica glass at 1064, 532, 355, and 266 nm was investigated. At 1064 nm, no difference in the LIDT was observed for all samples. In the range of 1064–355 nm, LIDTs of synthetic fused silica (SFS) were proportional to λ0.5, where λ is the wavelength. The LIDTs at 532 and 355 nm of fused quartz (FQ) and SFS containing 1000 ppm of Cl and no OH at 355 nm were slightly less than those of other SFSs. The mechanism of bulk damage at the 266 nm beam must be different from that at a longer wavelength, because the LIDT is considerably smaller than that of the value extrapolated from the λ0.5 dependence of SFS.
1884
Yu Yang, Shiji Jiang, Zihua Tian, Xinghui Wu, Chi Sheng and Xun Wang
Near band-edge photoluminescence was observed from strained and relaxed Si1-xGex/Si quantum wells grown by molecular beam epitaxy and annealed at 850–1100°C. Changes in the photoluminescence line energies were monitored, and the extent of both interdiffusion and relaxation in wells during annealing was calculated. Strain relaxation was observed only in quantum well structures annealed above 950°C. The experimental data confirmed the existence of an abrupt transition between stable and strain-relaxed Si1-xGex/Si quantum well structures, and it was also observed that photoluminescence was sensitive enough to detect the onset of strain relaxation in quantum well structures following rapid thermal annealing.
1889
Li Li, Zuowei Zuowei, Li Li, Jinan Jinan, Gao Gao and Suqin Suqin
The resonance Raman effect is produced in liquid-core optical fiber, enhancing the Raman spectral intensity 109 times. The absorption band and concentration of the sample effect the intensity of resonance Raman spectra. The optimum length of the optical fiber depends on the sample concentration. Good resonance Raman spectra of β-carotene in CS2 have been obtained and the intensity of the resonance Raman spectra has been enhanced 102–103 times. The Raman spectra of samples with low concentration (1×10-13 mol/L) have also been obtained. In the experiment, we have noted that the frequency deviation of the Raman line shifts when the concentration of β-carotene in CS2 is low.
1892
Yoshizo Kawaguchi Yoshizo Kawaguchi
Fractoluminescence and charge emission upon three-point-bending fracture of synthetic and natural quartz crystals have been studied. Broad luminescence bands centered at about 2.0, 2.9, and 5.0 eV have been observed in both cases. Time-resolved luminescence measurement could be performed on the 2.0 and 2.9 eV bands. The 2.9 eV band has a maximum intensity at about 5 ms after the fracture, and this band decayed within about 13 ms. On the other hand, the decay profile of the 2.0 eV band differed between synthetic and natural crystals. The 2.9 eV band might be due to the relaxation of the oxygen vacancy on the fracture surface, as in the case of silica glass. The 2.0 eV band seems to be due to an impurity center.
1897
V. Damodara Das and Laxmikant Damodare
The vacuum deposited thin films of n-CdSe0.7Te0.3 of 5000 Å thickness have been characterized by X-ray diffraction (XRD) for structural analysis, by energy despersive analysis of X-rays (EDAX) for compositional analysis and the scanning electron microscopy (SEM) for surface studies. Similar films have been deposited on Indium Oxide precoated microslide glass plates and the photoelectrochemical properties of n-CdSe0.7Te0.3/polyiodide junction are investigated for suitability for solar energy conversion by I–V measurements in the dark. Also, the carrier concentration and flat band potential have been calculated from the space charge capacitance vs voltage measurements. The minority carrier diffusion length, Lp has been determined using Gärtner's model. Using the Mott-Schottky plots, the energy band diagram at flat band condition has been constructed. The occurrence of high quantum efficiency and high power conversion efficiency have been explained.
1903
Hideyuki Iwata and Takashi Ohzone
The dependence of the conversion efficiency of rear locally-contacted p-type silicon solar cells on surface band bending at the rear Si–SiO2 interface is studied for several substrate resistivities and rear oxide thicknesses through two-dimensional device simulations. Conventionally, the cell efficiency was thought to increase as the band bending induced by work function difference and positive oxide charge increases. However, this is not necessarily true. Under the assumption of asymmetrical capture cross sections (σn/σp=102 at midgap) at the rear interface, the cell efficiency has a maximum value and then decreases gradually as the band bending increases. This is because a large number of generated electrons (minority carriers) are pulled into the rear surface and the greater part of the accumulated electrons flow into the rear p+-contact for large band bending.
1907
Toshio Kurobori Toshio Kurobori, Takashi Matsuki Takashi Matsuki, Karnati Somaiah Karnati Somaiah, Taku Kimura Taku Kimura, Shoichi Nakamura Shoichi Nakamura and Katsuyuki Inabe Katsuyuki Inabe
The stable and photostimulable F-aggregate centers, besides the already established isolated centers, located in the near IR region in BaFCl single crystals are reported. These F-aggregate centers are producible by two-photon excitation and the production rate can be enhanced by monovalent doping like incorporating K+ in BaFCl. The F-aggregate centers in BaFCl have been characterised by their growth behaviour, room temperature stability, optical bleaching, emission and the temperature dependence of the PSL lifetimes. It is a first time demonstration as applied to BaFCl single crystals to produce F-aggregate centers more efficiently by using the fourth harmonic of a Q-switched Nd:YAG laser as compared to X-irradiation.
1911
Hideki Hashimoto Hideki Hashimoto, Yoshiko Sawahara Yoshiko Sawahara, Yoshihiro Okada Yoshihiro Okada, Kingo Hattori Kingo Hattori, Tomokuni Inoue Tomokuni Inoue and Ryoka Matsushima Ryoka Matsushima
The crystal structure of all-trans-β-carotene was determined at 293 K. The space group determined in this investigation was consistent with that determined at 130 K by Senge et al. [Z. Naturforsch. C 47 (1992) 474]. Anisotropic displacements of lattice constants and molecular structures were observed upon raising the temperature from 130 K to 293 K. Photoinduced and time-resolved absorption spectroscopies were applied to all-trans-β-carotene single crystals. By exciting visible absorption bands of the crystals, we observed, for the first time, the photoinduced bleaching of infrared absorption bands. The bleaching typically showed a single-exponential recovery with a lifetime of ∼10 ms, which shows that some kind of metastable state is produced by exciting the visible absorption bands of the crystals. Depending on the crystals, however, we observed stretched-exponential and power-law recoveries. By inference based on the results for trans-polyacetylene, the cause of the latter two recoveries was attributed to the recombination of solitonlike excitations. Semi-empirical and ab initio molecular orbital calculations indicated the presence of solitonlike excitations in finite polyenes.
1919
Takefumi Oka, Kunihiko Tanaka, Taichi Tokunaga, Takashi Nakamura, Tomohiro Iiri and Makoto Yamazaki
Photoacoustic (PA) signals (amplitude and phase) from powdered samples are examined as a function of the effective absorption coefficient (k) of powder. Variation of the k value of a sample is accomplished by dilution of the sample in a diluent (BaSO4) with various degrees of dilution or by variation of the excitation wavelength for undiluted samples. It is determined that every powder studied shows a minimum in its PA phase vs k curve. A current theory of powder PA spectroscopy explains the presence of the phase minimum using a composite mechanism where the periodic expansion of buffer gas by heat transferred from the sample and the mechanical vibration of the sample are assumed as sources of the PA signal. The authors propose a method of estimating the relative value of k in a bulk sample from the phase minimum observed using the dilution method for the powdered sample.
1926
Hui-Chen Chang and Yen-Hwei Chang
A large Hall effect was observed in Fe–XCr–10Co (wt%) granular alloy films at room temperature. After aging, phase separation into α1 (ferromagnetic) and α2 (paramagnetic) phases was observed and verified using a high-resolution transmission electron microscope (HRTEM). The alloy composition and heat treatment conditions, which influence a film's microstructure, obviously affect the Hall effect. The Hall resistivity is positive for both as-deposited and annealed films. After aging the Fe–10Cr–10Co films at 200°C for 60 min, we observed the maximum Hall resistivity (ρH) of 12.6 µ Ω·cm (measured at 300 K and 14 kOe). The Hall resistivity varies almost linearly with the applied field.
1932
Hsiu-Fung Cheng Hsiu-Fung Cheng, Chen-Ti Hu Chen-Ti Hu, Yen-Yi Lin Yen-Yi Lin and I-Nan Lin I-Nan Lin
A core-shell microstructure is adopted to account for the unique resistivity-temperature (ρ–T) behavior of (Pb0.6Sr0.4)TiO3 materials prepared by the rapid thermal sintering (RTS) process. Instead of a V–shaped temperature coefficient of resistivity (VTCR) with critical temperature (T′c1) at around 220°C, commonly observed for the materials prepared by conventional sintering process, a ρ–T curve with single high Tc2\cong440°C is obtained. Moreover, the cooling rate after the RTS process markedly influences the ρ–T behavior. The apparent resistivity and the negative temperature coefficient of resistivity (NTCR) decrease as the cooling rate increases. The critical temperature (Tc2) for abrupt resistivity jump is insignificantly varied. These phenomena are ascribed to the modification of the thickness of the shell region due to the interdiffusion between the core and shell materials during the cooling stage. A simplified microstructural model is used to simulate the temperature dependence of resistivity and clearly explains the electrical behavior of these RTS samples.
1939
Tatsuyuki Shinagawa Tatsuyuki Shinagawa and Tsugunori Okumura Tsugunori Okumura
Hydrogen-related metastable defects (M3/M4) in n-GaAs were studied in relation to the EL2 center. We found that the M3/M4 defects were observed only in the crystals containing the EL2 center in the as-grown state after exposure to a hydrogen plasma. The EL3 level, which was tentatively assigned as off-center oxygen, could not be responsible for the formation of the M3/M4 defects. It was speculated that both diffused hydrogen and the pre-existing arsenic antisite or its related defects were responsible for the formation of the M3/M4 defects. A quantitative analysis with the samples exposed to atomic hydrogen showed that the M4 defect consisted of two different configurations. A metastable component of the M4 defect coupling with the M3 defect was not formed or latent in the as-irradiated state at room temperature. After bias annealing at higher temperatures, such as 420 K, the M3/M4 couple was formed.
1945
P. M. Borsenberger, E. H. Magin and S. A. Visser
Hole mobilities have been measured in di-p-tolylphenylamine doped poly(styrene) containing p-diethylaminobenzaldehyde diphenylhydrazone (DEH), an 0.32 eV trap. A DEH molar concentration of 10-5 decreases the mobility by a factor of two. For concentrations in excess of 10-5, the mobilities decrease with increasing concentration as approximately c-1.4, the field and temperature dependencies remaining essentially unchanged. For concentrations in excess of 10-1, transport is dominated by trap-to-trap hopping and the mobility increases with increasing trap concentration. The results are discussed within the framework of the Hoesterey-Letson formalism and the recent simulations of Wolf et al.. and Borsenberger et al..
1950
Vasile Tura, Liliana Mitoseriu, Constantin Papusoi, Toshio Osaka and Masanori Okuyama
Barium titanate ceramic samples of four different average grain sizes from 0.5 µm to 20 µm were studied by means of the ac calorimetric method. The ferroelectric-to-paraelectric transition temperature decreased with decreasing grain size. The temperature dependence of heat capacity showed hysteresis during a heating/cooling cycle. The thermal hysteresis was found to be grain-size dependent, with a possible maximum for grain sizes between 0.5 µm and 2.5 µm. The small shift of the Curie temperature detected in these ac calorimetry experiments suggests that internal stresses are the main cause of the observed grain-size effects.
1955
Sang-Shik Park, Su-Jin Chae and Soon-Gil Yoon
Microstructures and electrical properties of polycrystalline and oriented (Pb1-xLax)TiO3 (PLT) thin films deposited by rf magnetron sputtering using a ceramic (Pb0.7La0.3)TiO3 target having 20 mol% excess PbO were investigated. The grain size of oriented films deposited on La0.5Sr0.5CoO3(LSCO)/MgO was larger than that of polycrystalline PLT films on LSCO/Pt/Ti/SiO2/Si substrates. The dielectric constant and the dissipation factor of polycrystalline films measured at 10 kHz were 340 and 0.014, respectively. On the other hand, the dielectric constant and the dissipation factor of oriented films were 810 and 0.08, respectively. Both the polycrystalline and the oriented PLT films deposited at 500°C exhibited a paraelectric properties. The leakage current densities of the polycrystalline and the oriented PLT films were about 8.0 × 10-8 and 2.5 × 10-7 A/cm2 at 10 kV/cm, respectively.
1960
Kenji Ikuta Kenji Ikuta, Mitsuo Tsukada Mitsuo Tsukada and Hiroshi Nishimura Hiroshi Nishimura
Electron-cyclotron-resonance (ECR) plasma assisted deposition of strontium titanate (STO) thin films is discussed. Films having a high dielectric constant (εr) can be deposited at a temperature as low as 100°C by controlling the ECR plasma energy and ion current density. There exists a pressure that gives the maximum refractive index. The dependence of the refractive index and dielectric constant on the deposition temperature can be minimized at that pressure, where the ECR plasma energy and ion current density strongly assist the STO deposition. The pressure is approximately 0.05 Pa in an ECR sputter apparatus with a plasma energy of 10 eV and an ion current density of 5 mA/cm2. 100-nm-thick STO thin films, having εr of 70, a Qf product greater than 1000 in the mm-wave band up to 50 GHz, and dc leakage current less than 10-8 A/cm2 at 0.5 MV/cm, are realized by deposition at 0.05 Pa and 100°C. Deposition at other pressures results in a lower dielectric constant due to poor ECR plasma assistance. The properties of the STO thin films presented here are essential to process on-chip capacitors for monolithic microwave integrated circuits (MMICs).
1964
Tsutomu Ochiai
A piezoelectric accelerometer based on detecting piezoelectric charge Q1 caused by shear strain S5 has been developed, which consists of two piezoelectric elements made from a ferroelectric ceramic and one condenser element also made from a ferroelectric ceramic. Positive temperature dependence of dielectric constant of the former piezoelectric element (PbZr0.51Ti0.49O3 modified with 0.7 mol% Nb2O5) is compensated by negative dependence of the latter condenser element [Pb0.8La0.2(Zr0.4Ti0.6)0.95O3 or Pb0.7Sr0.2La0.1(Zr0.5Ti0.5)0.975O3] over a range of -50 to 300°C, with the result that sensitivity and its deviation are obtained to be 42×10-12 C/G and within 5%, respectively.
1970
Kinya Kato and Keiji Tanaka
Right- and left-handed polymer-dispersed cholesteric (chiral nematic) liquid-crystal (PDCLC) layers are stacked directly between a pair of substrates. Each layer in a device containing these stacked layers exhibits independent characteristics. This is because the PDCLC structure confines the liquid crystal (LC) within small cavities (droplets) surrounded by polymer, preventing LC mixing between layers. This technique makes PDCLC devices polarization free and effectively increases the reflectivity of such devices.
1974
Masaki Sei, Kohei Nagayama, Kotaro Kajikawa, Hisao Ishii, Kazuhiko Seki, Katsumi Kondo, Yoshiyasu Matsumoto and Yukio Ouchi
We demonstrated full determination of second-order nonlinear susceptibility of a 4′-n-octyl-4-cyanobiphenyl (8CB) liquid crystal (LC) monolayer adsorbed on a second-harmonic (SH) active polyimide (PI) substrate. In order to separate the SH signal of the LC film from that of the PI film, we adopted an interferometry technique of second-harmonic generation (SHG) using an ultra-thin film local oscillator. We have found a variety of phases in the components of susceptibility: those of χzii and χizi are almost the same but the phase of χzzz differs by 80° from the other two. The phases of the components of the surface susceptibility tensor are not always identical. This fact indicates that the surface SH response is more complicated than what we expected.
1982
Zhan He Zhan He, Ying Zhou Ying Zhou and Susumu Sato Susumu Sato
In order to determine 2-dimensional (2D) cell thickness and twist angle distributions in twisted nematic (TN) liquid crystal (LC) devices, we propose a 2D Stokes parameter method (2DSPM). A 2DSPM system is set up using a polarizing microscope, in which some preliminary experiments are conducted to demonstrate the validity of this 2DSPM. Experimental results of 2D distributions of cell thickness and twist angle in TN LC sample cells are given for the first time. The measurement accuracy of the 2DSPM system is analyzed.
1989
Koichi Tanaka Koichi Tanaka and Yasushi Ido Yasushi Ido
In this study, particle velocities and stresses in solid phase carbon dioxide were measured for pressures up to 500 MPa, using the split Hopkinson pressure bar method and the plate impact method. The particle velocities were measured using the electromagnetic induction method, while the stresses were measured using Polyvinylidene fluoride gauges. The shock Hugoniot is obtained mainly by employing the impedance match method. Also, some macroscopic change of the granular structure under shock loading was observed. The experimental results indicate that a transition from the shock compression curve to the isothermal compression curve occurs at around 110 MPa.
1994
Hiroyuki Fujishiro, Manabu Ikebe, Toshihiro Kashima and Atsuhiko Yamanaka
The thermal conductivity κ and thermal diffusivity α of high-strength polyethylene fibers, DyneemaTM, with various draw ratios were measured from 10 K to 260 K. κ and α increased with increasing draw ratio and α was nearly proportional to the square root of the tensile modulus E of the fiber. The estimated phonon mean free path l (40–60 Å) was almost temperature independent. Boundarylike scattering due to characteristic microstructures with comparable size to l may effectively limit the thermal conduction in these fibers.
1996
Kazushige Takechi, Tomoko Takagi and Setsuo Kaneko
This paper reports a study on the mechanism involved in depositing SiNx films at very high rates by using 40 MHz discharge SiH4/NH3/N2 plasma enhanced chemical vapor deposition (PECVD). The quality of the films is comparable to that of films deposited at low rates at a conventional 13.56 MHz frequency. From film deposition experiments, plasma diagnostic studies, and analytical calculation for both frequencies, we have found that the mechanism of depositing SiNx films at very high rates with a 40 MHz discharge can be explained by the higher dissociation efficiency of both NH3 gas and SiH4 gas than at a conventional 13.56 MHz. We also report the performance of a thin film transistor (TFT), applicable to LCD switching devices, that was fabricated with SiNx film deposited at the high rate of 350 nm/min with a 40 MHz frequency.
2002
Satoko Shinkai Satoko Shinkai, Katsutaka Sasaki Katsutaka Sasaki, Yoshio Abe Yoshio Abe and Hideto Yanagisawa Hideto Yanagisawa
We have investigated the initial silicide formation process of the single oriented (002) Hf film on (001) Si and compared it with that of the polycrystalline Hf film. From the results of X-ray diffraction analysis, we found that the first nucleation phase of Hf silicide is the multiphase silicides of Hf3Si2 containing a small amount of Hf5Si3 and the silicidation temperature is 420°C which is much lower than the values reported so far.The chemical nature of the silicide phase formed was evaluated by means of Auger electron spectroscopy and X-ray photoelectron spectroscopy. It is seen from these analyses that the chemical bonding state is the same as that of Hf3Si2, which has the lowest contact resistivity. Furthermore, it is also revealed that the diffusion barrier property of the single oriented (002) Hf film is superior to that of the polycrystalline Hf film, in which a rapid out-diffusion of Si occurs.
2007
T. Maeder, L. Sagalowicz and P. Muralt
Pt-based metallizations using different adhesion layers (Ti, Zr and Ta) were studied for use as electrodes for ferroelectric thin films on oxidized silicon substrates. Different ways of oxidizing the adhesion layers prior to ferroelectric film growth are compared, with regard to obtaining stable, adherent Pt films of well-defined (111) orientation, while avoiding lead diffusion through the electrode. Upon in-situ deposition of PbTiO3 at high excess lead flux, lead diffusion through the Pt film was found to depend strongly on the adhesion layer and the stabilization treatment. Pre-oxidation reduces lead diffusion during the later processing. Ti diffuses through the electrode upon oxidation, whereas Ta and Zr stay in place, in analogy to the diffusivities in the corresponding oxides. A novel oxidation treatment was developed to produce stable, adherent metallizations with controlled orientation and good barrier properties against lead diffusion.
2013
Hisao Sato, Tomoya Sugahara, Yoshiki Naoi and Shiro Sakai
The compositional inhomogeneity of the InGaN layers in GaN/InGaN/GaN double-hetero (DH) and InGaN/GaN single-hetero (SH) structures grown by metalorganic chemical vapor deposition (MOCVD) on sapphire (0001) and bulk GaN was investigated by means of cathodoluminescence (CL) and energy dispersive X-ray (EDX) spectroscopy. Dotlike CL image of the band edge emission from InGaN was observed. The bright spots were found to have higher indium content compared to that on the outside of the spots. The compositional inhomogeneity increased and the density of the spot decreased with increasing film thickness. Hexagonal hillocks, which had higher indium content and emitted stronger CL, were observed on the surface of the SH structure. Compositional inhomogeneity of homoepitaxial InGaN on bulk GaN substrate was much less compared to that of InGaN on sapphire revealing that dislocation plays a key role in producing an inhomogeneity. A possible mechanism that explains these phenomena is proposed.
2016
Dong-Wook Kim W. Noh
High-quality LiNbO3 thin films were grown by pulsed laser deposition (PLD) with a shadow mask. Epitaxial and twin-free films were obtained using a single crystal target without a post-annealing process. The film had a very smooth surface without the particulate problem, which is common in films grown by conventional PLD. The root-mean-square surface roughness was only 3.6 nm, and optical propagation loss was as low as 3 dB/cm.
2021
Cheol-Min Park, Moo-Sup Lim, Min-Koo Han and Yearn-Ik Choi
We propose a novel lateral field emission triode, which does not require any additional vacuum sealing process and exhibits superb field emitter triode performance. The purpose of this paper is to compare titanium polycide tip with polycrystalline silicon tip. A new experimental results of the device, such as variation of tip material, device stability experiment, measurement of the novel device in vacuum chamber in order to verify the proposed vacuum sealing process, and transconductance characteristics at each current level. The minimum turn-on anode to cathode voltage of titanium polycide tip is considerably decreased compared with polysilicon tip. The anode current measured in 10-8 Torr vacuum chamber is similar to the anode current measured in atmospheric pressure, which shows that the proposed vacuum sealing process is reliable. The stable current of 300 µA is maintained during 60 h.
2024
Akito Tanaka Akito Tanaka, Satoru Kishida Satoru Kishida, Yasuhiro Yamauchi Yasuhiro Yamauchi and Heizo Tokutaka Heizo Tokutaka
We treated Bi2Sr2CaCu2Oy (BSCCO) superconducting single crystals at various temperatures in air and investigated their surfaces with X-ray photoelectron spectroscopy. From the results, we determined that the carbon and oxygen impurities on the surfaces of BSCCO single crystals were removed by heating them in air at 400°C for 1 h. This was also confirmed by an Auger electron spectroscopy. In addition, the results of the half-width of the Cu-2p main peak and the intensity ratio of satellite to main peaks indicated that the optimum heat treatment temperature for obtaining a clean surface of BSCCO single crystal was approximately 400°C. The method is thought to be effective for cleaning the surfaces of superconducting oxides with various formations.
2028
Kouichi Tsuji, Toshihiko Nagamura and Kazuaki Wagatsuma
We measured the current passing between a sample and a scanning tunneling microscope (STM) tip under conditions of X-ray irradiation. As shown in our previous reports, this STM tip current originated from electron emission on the sample surface. For high precision STM tip current measurement, we applied an X-ray modulation technique using an X-ray chopper and a lock-in amplifier. X-rays modulated by the X-ray chopper irradiated the sample surface of the STM, and the STM tip current was detected using the lock-in amplifier. The largest and most stable output from the lock-in amplifier was obtained under the experimental conditions of low modulation frequency (∼10 Hz), strong X-ray intensity, and high STM bias voltage. Compared with measuring the STM tip current directly without the modulation technique, the precision of this measurement is threefold better.
2033
Masamichi Naitoh Masamichi Naitoh, Hiroshi Shimaya Hiroshi Shimaya, Akihiko Watanabe Akihiko Watanabe and Satoshi Nishigaki Satoshi Nishigaki
We report results of a scanning tunneling microscopy (STM) investigation of hydrogen-affected restructuring process at Si(111) surfaces. The hydrogen adsorption on the 7×7 surface produced clusters on the restlayer involving both Si adatoms from the initial dimer-adatom-stacking fault (DAS) structure and hydrogen atoms. Moreover, the restlayer was changed from the 7×7 to a 1×1-like structure by transferring dimer-walls. During the annealing process, the surface recovered the 7×7 structure via the formation of craters of bilayer depth. This is explained to be due to the local lack of Si atoms induced by migration-coalescence of the clusters at high temperatures.
2035
Sunil Wickramanayaka, Yunlong Li, Satoru Iizuka, Ken-ichi Takagi, Yukito Nakagawa, Tsutomu Tsukada and Noriyoshi Sato
The variation of the radial profile of plasma density with the excitation frequency was investigated using a magnetron-type plasma source. The plasma source is comprised of a cylindrical shaped rf electrode and two annular magnets attached to the outer surface of the rf electrode. As the excitation frequency of the plasma, 13.56 MHz, 40 MHz and 60 MHz were used. The radial profile of plasma density was observed in the downstream at 12 cm below the axial center of the rf electrode. Measurements were carried out for Ar plasma for pressures < 10 mTorr. The applied rf power varied from 200 W to 1500 W. The radial profile of the plasma density at a given distance from the axial center of the rf electrode changes with the change of excitation frequency. When the excitation frequency is 40 MHz, a radially uniform plasma could be obtained 12 cm below the axial center of the rf electrode. The nonuniformity of this plasma over an area of 300 mm diameter is <±5% regardless of the applied rf power. A change of pressure slightly affects the radial uniformity of the plasma. Plasmas produced by two other frequencies show a higher nonuniformity at the same distance from the axial center.
2039
Shin-ya Izumida, Kin-ya Onishi and Mitsunori Saito
Laser-induced breakdown of microparticles in ultrapure water was studied using a focused pulse laser of 532 nm wavelength. The transient acoustic signal generated by breakdown was detected on a nanosecond time scale using a fast-response polymer transducer. The temporal distribution of the acoustic pulses depends on not only the breakdown threshold of particles but also the spatial energy distribution of the laser beam around the focal point. The laser breakdown thresholds of various particles were estimated by analyzing the temporal distribution of the acoustic pulses. The breakdown threshold was higher in the order of silica, polystyrene, magnetite and gold particles.
2043
Miyako Matsui, Fumihiko Uchida, Kiyomi Katsuyama, Takafumi Tokunaga and Masayuki Kojima
Si(100) surface crystallinity after dry etching was measured using low-energy ion scattering spectroscopy (LEIS). We used 4-keV He+ ions as the incident beam, and neutral particles back-scattered at 180° were detected. A heavily damaged layer was observed immediately after reactive ion etching. After the heavily damaged layer was removed using a post-etch treatment, channeling and focusing effects were observed. The presence of a modified layer was confirmed even after the suboxide-rich layers were removed, because the channeling and focusing effects were slightly weaker than those of the surface without dry etching.
2051
Tetsuo Sakamoto Tetsuo Sakamoto, Zhaohui Cheng Zhaohui Cheng, Masanori Takahashi Masanori Takahashi, Masanori Owari Masanori Owari and Yoshimasa Nihei Yoshimasa Nihei
We are developing a novel three-dimensional (3D) microanalysis method by means of successive cross-sectional Auger mapping. In this method, a 3D elemental map will be obtained by repetition of the cross-sectioning of a sample using a gallium focused ion beam (Ga FIB) and Auger mapping of the cross section using an electron beam (EB). On the basis of this concept, an ion and electron dual focused beam apparatus was developed by combining a Ga FIB and a mass spectrometer with a scanning Auger microprobe. In this paper, we describe the concept and instrumentation of the dual focused beam apparatus. Two types of preliminary experiments; i) successive cross-sectioning of a microparticle (6.8 µmφ) and ii) successive cross-sectional sample current imaging of a bonding wire of an IC, demonstrated the capability to create flat analytical surfaces favorable for the 3D analysis with arbitrary shape and heterogeneity.
2057
Cheng-Hong Yu and Yee-Shyi Chang
The difficulty in the use of spin-on-glass (SOG) for multilevel interconnections leads to the requirement of higher-temperature (800–850°C) curing of the material, since the low-temperature annealed SOG may result in a significant amount of moisture during subsequent heat cycles leading to reliability problems. However, the application of an ion implantation method can improve the outgassing behavior of SOG annealed at 425°C. The temperature of the ion implantation treatment is made lower so as to be compatible with aluminum which is used as the conductive material. Ion implantation treatment using P+ (phosphorous) and As+ (arsenic) which are applied to the siloxane-type SOG is proposed in this paper. The thermal desorption analysis from experiments shows that the implanted SOG has a much lower water content and does not have a moisture desorption peak up to 600°C for both P+ and As+ implantations. The combination of the thermal curing and ion implantation treatments is beneficial for reducing the residual moisture content and promoting the thermal stability of SOG films. In addition, the results show that the implanted SOG is more insensitive to moisture absorption than the unimplanted SOG under the condition of 48-h air exposure. This implies that both water reabsorption and desorption performances of SOG can be further improved by ion implantation.
2062
Kazuya Nakanishi, Kimiyoshi Deguchi and Tadahito Matsuda
The patterning characteristics of synchrotron radiation lithography for hole patterns using a low-contrast mask (contrast: 3.5) are investigated. A resolution of 110 nm provides a large exposure dose latitude of more than 10% when the proximity gap is less than 15 µm, and the replicated minimum hole size is 70 nm with a 10-µm gap. Resist pattern sizes from 110 to 360 nm are kept within ±10% with proximity gaps of less than 20 µm. However, the exposure dose margin to guarantee mask linearity decreases to several percent because of the different optimum exposure dose for each pattern. Pattern size correction using mask bias to improve the mask linearity and exposure dose margin is proposed.
2066
Mitsunori Toyoda, Noboru Miyata, Mihiro Yanagihara and Makoto Watanabe
A laminar holographic grating was coated with a Mo/Si multilayer and the grating efficiency was measured between 27 and 35 nm for an incidence angle of 10°. The zero order was almost suppressed by the negative interference due to the groove profile. The maximum efficiency of first order was 4.8% at 31 nm. It was also found that the spectral wavelength provided by the grating at 10° incidence ranges from 28 nm to 32 nm.
2068
Kohzaburo Fujimoto Kohzaburo Fujimoto, Masashi Hirose Masashi Hirose, Kenji Inami Kenji Inami, Akimasa Ishikawa Akimasa Ishikawa, Iku Nagai Iku Nagai and Takayoshi Ohshima Takayoshi Ohshima
Using an oscilloscope as a differential amplifier, we built a simple and easily constructed system for wire-tension measurements by means of detecting the 3rd-harmonic signal of a mechanically vibrating wire, caused by an oscillating electric force.
2070
Hideyuki Takahashi, Ichiro Minato and Yuji Kondo
The peak shapes of F-Kα for fluorides with rare earth elements are examined using electron probe X-ray microanalyser (EPMA). It is demonstrated that the F-Kα spectra in fluorine compounds from 57La to 71Lu indicate characteristic peak shapes and the intensity ratios of the satellite Kα3,4 to the main Kα increase with the number of valence electrons.
2072
Naruhisa Miura, Akira Yamada and Makoto Konagai
An amorphous carbon (a-C) wire was directly deposited using scanning electron microscopy to determine a sub-micron gap in coplanar-type metal electrodes. The wire was employed to a lift-off mask for defining the gap between source and drain electrodes. By newly employing a ZnO buffer layer for removing the a-C wire, a gap size of 60 nm was successfully achieved. Moreover, this process was applied to fabricate a superconducting weak link device using a heavily phosphorous-doped Si thin film as a channel material.
2074
Keiko Suzuki, Taiji Nakae and Shigeki Mitaku
Outer membrane protein F (OmpF), porin, of Escherichia coli is an intrinsic membrane protein made of a β-sheet barrel, the amino acid sequence being as hydrophilic as many soluble proteins in spite of its location in the hydrophobic region of membrane. The binding of porin molecules with a lipid membrane and the flocculation of the protein were studied at various pH, using the combination of centrifugation and intrinsic fluorescence measurements. The binding of porin with the lipid membrane occurred in the pH range below 7, whereas the flocculation of porin in the absence of the membrane was observed only at pH below 5. Porin molecules in the pH range between 5 and 7 were stable as a colloid but spontaneously bound with the lipid membrane soon after the addition of lipid vesicles. The possible mechanism of the structural formation of porin in the outer membrane was discussed based on the pH dependence of the membrane binding ability of this protein.