Featured Articles

Corrosion in Advanced Nuclear Reactors

and

© Copyright 2021 by The Electrochemical Society.
, , Citation Gary S. Was and Todd R. Allen 2021 Electrochem. Soc. Interface 30 57 DOI 10.1149/2.F10212IF

1944-8783/30/2/57

Abstract

Commercial nuclear power plants in the United States are light water reactors (LWRs) that use water as a coolant, with temperatures ranging between 280°C and 320°C. Water purity is tightly controlled; nevertheless, the high temperatures expose components in the water circuit to degradation by corrosion by many different types of environmental attack. Uniform corrosion occurs across the entire surface of a material and is prevalent in engineering systems to some extent. Site-specific corrosion processes, such as crevice corrosion, intergranular attack, or galvanic corrosion, are common in complex engineering systems that consist of multiple materials joined by welds or other solid state joining processes. Even within a single component, if second phase strengthening is used or if surface defects are present, localized corrosion can occur.

Export citation and abstract BibTeX RIS

10.1149/2.F10212IF