Abstract
Ca-substituted Li0.44MnO2 samples were prepared from the Na-analogs via Na/Li ion-exchange in molten LiNO3 at 270°C. The Ca substitution was confirmed by using XRD, EDX and ICP analyses in not only the precursor sodium compounds but also the ion-exchanged samples. The electrochemical measurements between 2.0 and 4.8 V showed that the initial discharge capacity decreased from 187 mAh g−1 to 127 mAh g−1 due to the Ca substitution. On the contrary, the cycling performance was drastically improved by the Ca substitution; the discharge capacity retention rate increased from 72% in unsubstituted Li0.28MnO2 to 85% in Li0.24Ca0.05MnO2 after 50 cycles. The dQ/dE plots clearly indicated the decrement of the insertion and extraction reaction in the 4 V range by the Ca-substitution.
Access this article
The computer you are using is not registered by an institution with a subscription to this article. Please choose one of the options below.