Abstract
The bond strength of plasma-enhanced tetraethyl-orthosilicate (PE-TEOS) oxide, bonded and annealed at low temperatures (
and below), is enhanced using a thin layer of high-κ dielectric at the bonding interface. Before bonding, various thin
capping layers of high-κ dielectrics (
,
, and
) are deposited separately on polished PE-TEOS wafers, followed by surface activation. After a
anneal in
ambient for 3 h, the bond strength of wafer pairs bonded with PE-TEOS oxide is enhanced by 97.9, 73.3, and 31.0%, respectively, with
,
, and
layers at the interface.
Access this article
The computer you are using is not registered by an institution with a subscription to this article. Please choose one of the options below.