This work investigates the interaction of Equation or symbol description not availablePt∕HfO2∕Si nanometric film structures with deuterium gas Equation or symbol description not available(H22) at Equation or symbol description not available500°C, simulating the hydrogen passivation step commonly applied to metal-oxide-semiconductor devices. Selective chemical etching of Pt and Equation or symbol description not availableHfO2 combined with Equation or symbol description not availableH2 detection by nuclear reaction analysis allowed quantification and depth profiling of Equation or symbol description not availableH2 incorporated into the structures. The presence of the top Pt layers does not measurably affect Equation or symbol description not availableH2 amounts incorporated underneath. However, Equation or symbol description not available∼1014H2cm−2 are trapped at the Equation or symbol description not availablePt∕HfO2 interfaces. This interfacial Equation or symbol description not availableH2 trapping implies that conventional Equation or symbol description not availableH2 passivation annealing can substantially influence the chemistry of metal–Equation or symbol description not availableHfO2 interfaces.