The present study examines the influence of surface pretreatment on the evolution of nanotubular (T) and nanoporous (P) oxide film morphologies on titanium foil anodized potentiostatically, at Equation or symbol description not available20V, in fluoride-containing Equation or symbol description not available1M Equation or symbol description not availableH3PO4 electrolyte. The foil was used in the untreated, mechanically/chembreically polished or preanodized conditions. The preanodization resulted in fluoride-free barrier films. Mainly T regions were produced on polished foil during subsequent anodizing in fluoride-containing Equation or symbol description not available1M Equation or symbol description not availableH3PO4 electrolyte. In contrast, the P regions dominated on polished foil preanodized to Equation or symbol description not available20V. Both P and T regions resulted with rolled foil preanodized to Equation or symbol description not available20V or polished foil preanodized to Equation or symbol description not available10V. Raman spectroscopy disclosed anatase and rutile at P regions, whereas T regions are mainly amorphous. The P film thickened at a constant rate of Equation or symbol description not available6×10−2nms−1, while the T film reached a limiting thickness of Equation or symbol description not available∼700nm due to the relatively high solubility of the amorphous oxide. The presence of P film resulted in increased currents during anodizing. Furthermore, the results suggest that the formation of T film depends upon the access of Equation or symbol description not availableF− ions to the titanium/film interface, resulting in the stabilization of a mainly amorphous film structure.