The electrical characteristics of titanium dioxide films grown on p-type indium phosphide substrate by metallorganic chemical vapor deposition (MOCVD) were studied. For indium phosphide with ammonium sulfide treatment, the electrical characteristics are improved due to the reduction of interface state density. The electrical characteristics can be further improved by postmetallization annealing. The hydrogen from the postmetallization annealing process can passivate the defects and the grain boundaries of polycrystalline Equation or symbol description not availableTiO2 film. The leakage current densities can reach 2.7 and Equation or symbol description not available2.3×10−7A∕cm2 under positive and negative electric fields at Equation or symbol description not available1MV∕cm, respectively. The dielectric constant and effective oxide charges are 46 and Equation or symbol description not available1.96×1012C∕cm2, respectively. The interface state density is Equation or symbol description not available7.13×1011cm−2eV−1 at the energy of Equation or symbol description not available0.67eV from the edge of valence band.