The film responsible for passivity when iron is immersed in concentrated nitric acid is shown to be ferric acid or a related higher valence iron compound. This was proved (a) by demonstrating formation of chromates when a 2.84% Cr‐Fe alloy is passivated, (b) by showing complete suppression of the iron‐nitric acid reaction when iron is previously immersed in potassium ferrate solution, and (c) by immersing passive iron in
solution and observing higher valence iron compounds displaced from the surface by adsorbed OH−. The maximum of
that was found is the same order of magnitude as moles chromate adsorbed on iron from chromate solutions as reported by other investigators. This amount of ferric acid, when it decomposes, is calculated to form a film of ferric oxide 40–125 Aå thick, which thickness range agrees with that of residual oxide films on passive iron measured previously by others.
The higher valence iron compound forms at anodic areas of the iron surface during the iron‐nitric acid reaction. When sufficient local concentration is achieved, the compound adsorbs (chemisorbs) on iron, satisfies metal surface affinities, and is itself stabilized against decomposition by adsorption. The metastable compound breaks down by cathodic reduction, mechanical shock, or presence of halide ions, the latter either displacing the adsorbed compound or hastening its decomposition. The roles of urea and hydrogen peroxide in nitric acid are discussed.
Access this article
The computer you are using is not registered by an institution with a subscription to this article. Please choose one of the options below.