To investigate extrinsic and intrinsic behavior of the semiconductor Equation or symbol description not availableCuInTe2, high‐temperature electrical resistivity experiments were carried out, using the technique of porcelain “cocoons.” Equation or symbol description not availableCuInTe2 was considered as part of the pseudobinary system Equation or symbol description not availableCu2Te‐In2Te3. Inspection of the plots 1n ρ vs. 1000/T for samples with 44 to 56 molar% Equation or symbol description not availableCu2Te revealed the existence of two extrinsic regions: room temperature to 200°C and 200°–710°C. The latter was found complex and exhibited in general two different slopes. The intrinsic region in these samples existed in a narrow temperature interval between 710° and 779.8°C (the melting point of Equation or symbol description not availableCuInTe2), and was well denned and reproducible. Assuming a Equation or symbol description not availableT−3/2 dependence of carrier mobility, the “thermal” energy gap of Equation or symbol description not availableCuInTe2 could be calculated from the intrinsic slopes in the plots In Equation or symbol description not availableρ vs.1000/T, and was found to be 1.04 ev. Observed deviations from this value were ±0.02 ev. Prolonged annealing of various samples of Equation or symbol description not availableCuInTe2 at 400°promoted disappearance of extrinsic differences among them, while their intrinsic slopes remained the same.