Passive films were formed on a high purity Fe‐23 Cr alloy in acid sulfate solutions in the presence and absence of chloride ion. The resulting film composition was investigated by Auger depth profiling. The passivated samples were exposed to a 1M
solution at a constant potential slightly above the critical pitting potential, and the current‐time transient was measured in order to compare the relative stability of the different films. The results obtained suggest that the formation conditions influence the chloride content of the passive film and the breakdown behavior. Passive films formed in the presence of chloride contain chloride and are slightly less stable towards breakdown. No chloride was found in films formed in sulfate and subsequently exposed to chloride well below the pitting potential.