A series of experiments have been carried out to characterize the perfection of silicon wafers oxidized in an accelerated manner at 700°C and 20 atm steam, All experiments were performed using 3 in. diam wafers. High pressure steam oxidations of (100) and (111) oriented silicon, both n and p type, resulted in suppression of oxidation‐induced stacking faults for all thicknesses studied (up to 5 μm oxide). Some wafers were subjected to normal 1 atm steam oxidations to produce stacking faults and subsequently steam oxidized at high pressure to study the behavior of these preexisting stacking faults. Results showed some shrinkage, but less than might be expected based solely on the consumption of silicon. Capacitance transient measurements have been made on the high pressure steam‐oxidized samples and compared to wafers treated at higher temperatures at 1 atm. The defect‐state concentration after high pressure steam oxidation was found to be nearly identical to the preoxidation condition.