At temperatures above the melting point of lithium, anodes of lithium‐boron alloys consist of a solid porous structure filled with nearly pure liquid lithium. The anodes are capable of being discharged at 4 A/cm2 and −3V (vs.a chlorine reference electrode). During discharge, there are two very negative voltage plateaus with a small difference in voltage between them. At 8 A/cm2the change in voltage over the combined plateaus is ±12% of the average voltage for the plateaus. The first plateau is terminated at three different anode compositions (Equation or symbol description not availableLi6B, Equation or symbol description not availableLi4B, and Equation or symbol description not availableLi3B) depending on the initial anode composition. The second plateau is terminated when the anode's composition corresponds to Equation or symbol description not availableLi2B. A more positive portion of the voltage curve terminates when the anode's composition corresponds to Equation or symbol description not availableLi7B6. An alloy of 86 atomic percent (80 weight percent) lithium has a capacity of 7.6 MC/kg and 5.3 GC/m3. The alloys have superior lithium retention at 873°K compared with lithium‐filled, nickel Feltmetal.