A gettering technique which prevents microdefect formation during oxidation processes after the growth of reduced pressure Si epitaxial layer for bipolar devices is described. A gettering process which consists of protection of the back damage layer with Equation or symbol description not availableSi3N4 film is proposed. A microdefect density in epi‐layers of ∼102 cm−2 is obtained by back damage with the Equation or symbol description not availableSi3N4 film coating technique, on the contrary, the microdefect density reaches ∼106 cm−2without the Equation or symbol description not availableSi3N4 film. The critical thickness of Equation or symbol description not availableSi3N4 film to elminate microdefects in epi‐layers is obtained 2500 and 200Å for substrates without and with back damage, respectively. It is found that the gettering action is closely correlated with induced defects in the back surface (OSF, dislocation, damage line, etc.) by sandblast‐damaging and/or Equation or symbol description not availableSi3N4 film.