Abstract
The cyanoaurate (III) ion has been found to form and accumulate in acidic or neutral gold plating baths containing cyanoaurate(I) as the source of gold. This trivalent gold species brings about a decrease in plating current efficiency because its reduction to gold metal requires three faradays per mole, whereas only one faraday is consumed to reduce one mole of Au (I). The accumulation of Au (III) should therefore be minimized to produce gold deposits with a thickness unaffected by bath age. This paper describes various methods for achieving this objective, which include the use of the so‐called “dimensionally stable anode” and a techniqe of chemically reducing Au (III) to Au (I).