Complex plane impedance diagrams were used to determine the ionic conductivity of Fe‐doped β‐alumina over the composition range Equation or symbol description not availableNa1.3Al9.86‐Fe1.14O17.15(10% Fe by weight) to Equation or symbol description not availableNa1.3Al7.18Fe3.82O17.15 (30% Fe by weight). The influence of starting material [Equation or symbol description not availableFe2O3, Equation or symbol description not availableFe2(C2O4)3·6H2O, Equation or symbol description not availableFe(C2O4)·2H2O,Equation or symbol description not availableFe(NO3)3·9H2O] upon grain boundary and bulk properties was studied. The ionic conductivity of all doped materials increased over that of undoped β‐alumina. The best materials obtained resulted from doping with Equation or symbol description not availableFe(C2O4)·2H2O. At the 10% doping level, bulk conductivity reached a maximum coinciding with a minimum in activation energy. Electronic conductivity was investigated by a “floating” blocking technique. The electronic conductivity was small at the 15% dopant level, representing <10−3% of the total conductivity, but increased rapidly and at the 30% dopant level was ∼0.1% of the total conductivity. Preliminary Mössbauer studies showed a steady increase in the Fe(III)/ Fe(II) ratio as dopant levels increased.