When luminescent screens are manufactured for color TV tubes, various layers are applied successively to the glass screen. The bonding of the layers to the screen glass and to each other is caused by various forces. These interaction forces affect the adhesion of the different interfaces. The adhesion mechanism of the precoating, phosphor, and lacquer layers and the aluminum backing before and after baking out the luminescent screen are discussed.