Abstract
Low temperature sublimation is shown to significantly reduce the metal and ‒P‒OH containing impurity levels of practical‐grade phosphorus oxychloride. Regular distillation and sub‐boiling distillation are also effective for removing ‒P‒OH impurities and provide products with 114–119 ppm of residual ‒P‒OH. The purification efficiencies of these physical methods are compared with that resulting from chemical treatment to convert ‒P‒OH impurities into other species. A method based on chemical reaction followed by low temperature sublimation is described for removal of
from practical‐grade material and reduction of trace materials to low ng/ml levels.
Access this article