Polarization behavior of the Ni‐200 electrode in Equation or symbol description not available75%Na2S‐25%FeS at 1000°C under Equation or symbol description not availableH2‐0.32%H2S at 1 atm is linear over an overpotential range of Equation or symbol description not available−600≥η≥600 mV and is consistent with resistance polarization in the electrolyte. Similar polarization behavior of the 304 stainless steel electrode and of the Ni‐200 electrode in Equation or symbol description not available85%Na2S‐15%NiS suggests that the charge transfer mechanism is a sulfide/polysulfide exchange reaction. Nonelectrodic dissolution of nickel in the Equation or symbol description not available75%Na2S‐25%FeS melt occurs at Equation or symbol description not available1.6×10−6 g cm−2 s−1, apparently due to oxidation by Equation or symbol description not availableH2S. Anomalously high dissolution rates are attributed to trace polysulfide.