Abstract
Electroactive polyaniline can be prepared in nonaqueous solutions (such as propylene carbonate (PC), acetonitrile
) containing 1.0 mol dm−3 aniline tetrafluoroborate (ATFB). The polyaniline prepared in PC containing 1.0 mol dm−3ATFB showed a high discharge capacity compared with that prepared in 2.0 mol dm−3
aqueous solution containing 1.0 mol dm−3 aniline (pH 1) because oxidative degradation during the electropolymerization did not occur in PC containing 1.0 mol dm−3 ATFB. However, the decrease in the discharge capacity of polyaniline prepared in PC containing 1.0 mol dm−3ATFB with increasing discharge current was larger than that prepared in 2.0 mol dm−3
aqueous solution containing 1.0 mol dm−3 aniline (pH 1). From scanning electron microscopic observations, it can be seen that these polyanilines have different morphologies.
Access this article