The exchange current density Equation or symbol description not available(i0) for oxygen reduction has been measured by using a potential step technique on nonporous oxide electrodes in an Li/K(62/38 mole percent) carbonate eutectic melt at 923 K. Nonporous oxides were fabricated by a hot isostatic pressing method to be as dense as possible to study the kinetic parameters of the oxygen reduction on smooth oxide electrodes. However, the nonporous oxides had slightly rough surfaces. Accordingly, to allow for electrode roughness, the area of the nonporous oxide electrodes were corrected from the double‐layer capacity values to make a comparison between our nonporous oxide electrodes and those used by other researchers. Results were obtained onEquation or symbol description not availableLi0.1Ni0.9O, Equation or symbol description not availableLiFeO2, Equation or symbol description not availableLiCoO2, and Au electrodes under Equation or symbol description not availablepO2/pCO2=0.9/0.1, Equation or symbol description not availablepO2/pCO2=0.33/0.67, and Equation or symbol description not availablepO2/pCO2=0.14/0.30 (70% air and 30% Equation or symbol description not availableCO2) atmosphere. A typical result for the exchange current density was as follows: 74 mA/cm2 on Equation or symbol description not availableLi0.1Ni0.9O, 9 mA/cm2 on Equation or symbol description not availableLiFeO2, 11 mA/cm2 on Equation or symbol description not availableLiCoO2, and 9 mA/cm2 on Au at 923 K under the Equation or symbol description not availablepO2/pCO2=0.9/0.1 atmosphere.