Chemically assisted ion beam etching, using Ar+ ions and Equation or symbol description not availableCl2 as the reactive gas, has been investigated for the etching of common materials used in silicon‐based microfabrication: Equation or symbol description not availableSiO2, Equation or symbol description not availableSi3N4, single‐crystal Si, and polycrystalline Si. Two possible etch masks for etching the Si substrate have been characterized: Equation or symbol description not availableSiO2 and Equation or symbol description not availableTiW. Etch rates for all these materials and Si etch profiles have been studied as a function of ion energies from 300 to 1000 eV, current densities between 0.05 and 0.15 mA/cm2, and reactive Equation or symbol description not availableCl2 flow rates at substrate temperatures of 30 and 85°C. Trenches etched into Si using Equation or symbol description not availableTiW as a mask showed steeper profiles and less enhanced etching in the bottom corners than those with an Equation or symbol description not availableSiO2 mask. These etch effects are attributed to a deposited layer on the trench sidewalls, when using Equation or symbol description not availableTiW as a mask. This Si etch process has important applications in shallow trench isolation for deep submicron complementary metal oxide semiconductor integrated circuits.