Stoichiometric Equation or symbol description not availableLi4Mn5O12 spinel oxide has been synthesized by an oxidation of Equation or symbol description not availableMn2+ by lithium peroxide in the presence of excess lithium hydroxide followed by firing at T ⩽ 500°C. The sample has been characterized by X‐ray diffraction, elemental and oxidation state analyses and thermogravimetric analysis. X‐ray results indicate that Equation or symbol description not availableLi4Mn5O12 begins to disproportionate at T > 500°C to give Equation or symbol description not availableLi1+xMn2−xO4 (x < 0.33) and Equation or symbol description not availableLi2MnO3. The samples fired at 400 and 500°C show in the voltage range 3.3–2.3 V, an initial capacity of 160 and 153 mAh/g, respectively, which is close to the theoretical value. The sample fired at 500°C shows excellent cyclability with <2% capacity decline over 40 cycles.