Abstract
Microfabricated
nanotips are potentially useful as scanning tips in near-field optical microscopy and sensor related functions. We report a process in which the rounding nature of isotropic etching combined with undercutting property of Si(100) are effectively used to microfabricate laterally ordered
nanotips. Combination of excessive isotropic wet etching of thermally grown
with anisotropic etching of n-type silicon along 〈100〉 planes leads to the formation of nanotips with sharpness ∼15 nm. Uniform periodic array of nanotips form due to coalescence of excessively etched
resulting in nanotips length ⩽ the separation between the original photolithographic features. Finally, the overall process of nanotip formation is discussed by considering the roles of rapid isotropic etching of
in buffered oxide etch solution, anisotropic etching of Si〈100〉 in KOH solution, and slow
etching in KOH solution. © 2003 The Electrochemical Society. All rights reserved.