A simple fabrication method of 2D Equation or symbol description not availableSiO2 corrugated layers and their suitability to enhance output coupling efficiency of a ZnS:Tb thin-film phosphor layer in an anode part of field emission display (FED) devices is discussed. For patterning of 2D dotted arrays of Equation or symbol description not availableSiO2 films, we used two-step irradiated hologram lithography and reactive ion etching. The formation of a wavelength-scale uniform 2D Equation or symbol description not availableSiO2 dotted array was confirmed by morphological analysis. We presented the finite-difference time-domain analysis for calculating the output light resulting from the insertion of a 2D Equation or symbol description not availableSiO2 corrugated layer into the interface between the glass substrate and the ZnS:Tb thin-film phosphor. A significant enhancement (a factor of 4.0-4.7) of the output coupling cathodoluminescence (CL) efficiency is reported in the low-voltage (0.5-4.5 kV) characteristics under electron-beam excitation for the ZnS:Tb thin-film phosphor deposited on a 2D Equation or symbol description not availableSiO2 corrugated substrate. The computational analysis, CL characterizations, and far-field measurement demonstrated that the 2D Equation or symbol description not availableSiO2 corrugated substrate served as diffraction scattering layers, increasing the output coupling efficiency, which is critically important for development of commercial FEDs employing thin-film phosphors. © 2003 The Electrochemical Society. All rights reserved.