Dynamic aspects of Equation or symbol description not availableLi+ intercalation-deintercalation into single KS-44 carbon particles (8-50 μm in diameter) embedded in thermally annealed Ni foils were examined in 1 M Equation or symbol description not availableLiClO4, ethylene carbonate (EC), diethyl carbonate (DEC) (1:1 v/v) solutions by in situ, time-resolved Raman microscopy. A direct correlation was found between the position of the prominent G band, in the range 1581-1590 cm−1, and the amount of Equation or symbol description not availableLi+ in KS-44 within the so-called dilute stage 1 phase. This information was used to determine spectroscopically and in real time the average concentration of Equation or symbol description not availableLi+ within the volume of the particle probed by the laser beam following application of a potential step between 0.05 V vs. Equation or symbol description not availableLi/Li+, i.e., nominally full Equation or symbol description not availableLi+ intercalation and 0.7 V vs. Equation or symbol description not availableLi/Li+, i.e., full Equation or symbol description not availableLi+ deintercalation. Quantitative analysis of these transient data based on a spherical diffusion model yielded a time constant for Equation or symbol description not availableLi+ deintercalation for dilute stage 1 phase consistent with reported values of Equation or symbol description not availableLi+ diffusion coefficients within graphitic materials and the size of the particles probed. Single KS-44 particles cycled repeatedly into the deep Equation or symbol description not availableLi+-intercalation region recorded at high potentials Equation or symbol description not availableE>0.5V vs. Equation or symbol description not availableLi/Li+, displayed a new Raman band attributed to bounding graphite layers not observed for pristine KS-44 carbon under otherwise identical conditions. This new spectral feature has been tentatively associated with chemical modifications of the carbon itself which may be at least partially responsible for irreversible capacity losses. © 2002 The Electrochemical Society. All rights reserved.