The formation of Equation or symbol description not availableLiCo2O4 spinel oxide has been investigated by chemically extracting lithium with the oxidizing agent Equation or symbol description not availableNa2S2O8 from three samples of Equation or symbol description not availableLiCoO2 that were synthesized at 400, 600, and 800°C to obtain Equation or symbol description not availableLi0.5CoO2, followed by heat-treatment at 200°C. The samples have been characterized by X-ray diffraction, atomic absorption spectroscopy, and a redox titration to determine the oxygen content. While the Equation or symbol description not availableLi0.5CoO2 sample obtained from the Equation or symbol description not available400°C Equation or symbol description not availableLiCoO2 crystallizes in the normal cubic spinel structure with a cation distribution of Equation or symbol description not available(Li)8a[Co2]16dO4, that obtained from the Equation or symbol description not available800°C Equation or symbol description not availableLiCoO2 maintains the layer structure even after heating at moderate temperatures. The voltage profile of the Equation or symbol description not availableLiCo2O4 spinel has been investigated experimentally. While the extraction of lithium from the 8a sites occurs at around 3.8-4 V, the insertion of lithium into the 16c sites occurs at around 3.5-3.6 V. The experimentally observed voltage difference of 0.3 V between the two processes is much smaller than that predicted from theoretical calculations (1.3 V) in the literature and observed for the Equation or symbol description not availableLiMn2O4 system (1 V). © 2002 The Electrochemical Society. All rights reserved.