An Equation or symbol description not availableLiCoO2 thin‐film cathode was deposited onto sintered alumina and Equation or symbol description not availableSi/SiO2 substrates. After annealing at Equation or symbol description not available800°C in Equation or symbol description not availableO2 for Equation or symbol description not available30min, the film deposited on alumina consisted of large particles with several cracks, whereas the film deposited on the Equation or symbol description not availableSi substrate was composed of very small and uniform particles. The films deposited on Equation or symbol description not availableSi showed improved electrochemical properties, such as peak potential divergence and rate capability, over those for the alumina substrate electrode, which can be attributed to differences of the particle size, surface morphology, and the low electrical resistance of the current collector. ©1999 The Electrochemical Society