Texture improved Equation or symbol description not availableTiN films were prepared by a two‐step deposition process. A thin uncollimated Equation or symbol description not availableTiN layer is deposited first at low substrate temperature and sputtering power. This layer has poor step coverage and high resistivity, but acts as a crystallographic seed layer for the subsequent collimated Equation or symbol description not availableTiN layer deposited at high substrate temperature and sputtering power. The Equation or symbol description not availableTiN layer stack is deposited sequentially without vacuum break. The resulting Equation or symbol description not availableTiN layer has a low resistivity of Equation or symbol description not available72.25 μΩ cm, high 〈111〉 preferred orientation, and improved bottom coverage in sub‐quarter‐micrometer contact holes and trenches. ©1999 The Electrochemical Society