Abstract
We report on the deposition of Ti1-xAlxN films by chemical vapor deposition (CVD) system. Titanium tetrachloride (TiCl4), dimethylethylamine alane (DMEAA) and ammonia gas were used as sources. Chemical composition, microstructure and electrical resistivity were investigated at various deposition conditions by X-ray photoelectron spectroscopy, X-ray diffraction, scanning electron microscopy and 4 point probe. Al content, x, in Ti1-xAlxN film was varied from 0.04 to 0.79 in our experimental conditions. As deposition temperature increased in the temperature range from 220°C to 410°C, Al content decreased. Also, Al content in Ti1-xAlxN films shows a linear relationship with the partial pressure of DMEAA. Up to x=0.15, glancing angle XRD peaks showed only B1 (NaCl) cubic structures but further increasing of Al content leads to amorphous structure. For Ti0.76Al0.24N film, Cu(50 nm)/Ti0.76Al0.24N(20 nm)/Si substrate stack was prepared to examine the barrier property against Cu diffusion. Cu diffused into Si substrate through the Ti0.76Al0.24N(20 nm) film from 700°C, 30 min vacuum annealing. This result is higher than that of CVD-TiN(50 nm) barrier which failed at 400°C.
Access this article
The computer you are using is not registered by an institution with a subscription to this article. Please choose one of the options below.