Abstract
The paper deals with the physical properties of colloidal silica dispersed system such as distribution width (Qx, %) and density (qx, %) defined by photon cross correlation spectroscopy (PCCS) at an average size of 17.06 nm for D50 % and the area of specific surface of 349.96 m2 cm−3 depending on molar (Rm2) optimal ratio of silica stone mineral to alkali ash powder. The change of crystal structure to amorphous state was determined by X-ray diffraction analysis. The results of their kinematic viscosity, liquid density, UV light adsorption inspections show possibility to produce the colloidal silica by using the wetting and ultrasonic vibration method for that fusible alloy.
Export citation and abstract BibTeX RIS
Content from this work may be used under the terms of the Creative Commons Attribution 3.0 licence. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.