The effects of Alkanolamide (ALK) addition on swelling, rheometric and tensile properties of unfilled chloroprene rubber (CR) compounds were investigated. The ALK was prepared from Refined Bleached Deodorized Palm Stearin and diethanolamine and -together with magnesium and zinc oxides- incorporated into the CR compounds. The ALK loadings were 0.5, 1.0, 1.5 and 2.0 phr. It was found that ALK enhanced the cure rate and torque difference of the CR compounds. ALK also enhanced the tensile modulus and tensile strength; especially up to a 1.5 phr loading. The swelling test proved that the 1.5 phr of ALK exhibited the highest degree of crosslink density which caused the highest in tensile modulus and tensile strength.