Abstract
Research of modifying particle board has been prepared by mixing of pinus merkusii sawdust and rice husk, where used of adhesive base on Boiled Soybean Water (BSW) has been done. The research utilize the rise husk and sawdust pines mixed, and used of a renewable and environmental adhesive to replace the toxic and carcinogenic one. The testing of adhesive included are; colour, pH, solid contain, gelatination time, density and viscosity. Result showed yellowish colour, 10 of pH, 44.70 % of solid contained, 56.29 minutes of gelatination time, and 1.1656 g/cm3 and 182.4387 cP of viscocity respectively. While the particle boards testing include are density, moisture, immersion, thickness, Modulus of Rapture (MOR) and Modulus of Elasticity (MOE). The particle board best ratio it was 1:4 (Rice husk: pinus merkusii sawdust). Result of each parameter are, 0.7735 g/cm3 of density, 5.79 % of moisture, however the immersion for 2 hours is 26.90 % and immersion for 24 hours is 39.77 %, 101.1592 kg/cm2 of MOR and 18,248.3063 kg/cm2of MOE.
The summary, the adhesive based on SNI 06-4567-1998 and the particle board based on SNI 03-2105-1996
Export citation and abstract BibTeX RIS
Content from this work may be used under the terms of the Creative Commons Attribution 3.0 licence. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.