Paper The following article is Open access

Growth of PEO ceramic coatings on AA 2024-T3 aluminium alloy

, and

Published under licence by IOP Publishing Ltd
, , Citation S Forero Sotomonte et al 2016 J. Phys.: Conf. Ser. 687 012037 DOI 10.1088/1742-6596/687/1/012037

1742-6596/687/1/012037

Abstract

The growth of PEO ceramic coatings on AA 2024-T3 aluminium alloy in an aqueous Na2SiO3 (10.5g/l), KOH (2.8g/l) solution at 310 and 400V for 500 and 710s, was investigated. The morphology, roughness and thickness of the coatings were determined by SEM, digital microscopy, XRD diffraction analysis and thickness measuring instrument. The results show that thicker coatings are produced with longer process times and high applied voltages. Due to the nature of the PEO process, the roughness of the surface coatings increases as the coating become thicker, due to the development of sparks. The coatings are porous, with a crater like morphology and they are mainly amorphous.

Export citation and abstract BibTeX RIS

Content from this work may be used under the terms of the Creative Commons Attribution 3.0 licence. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.

Please wait… references are loading.
10.1088/1742-6596/687/1/012037