Erratum The following article is Free article

Erratum: Fabrication of highly conductive polyester fabrics using single-wall carbon nanotubes inks for EMI shielding [Jpn. J. Appl. Phys. 63 04SP01 (2024)]

, , , , , , , and

Published 23 April 2024 © 2024 The Japan Society of Applied Physics
, , Special Issue on Microprocesses and Nanotechnology 2023 (MNC2023) Citation Yuito Horita et al 2024 Jpn. J. Appl. Phys. 63 049401 DOI 10.35848/1347-4065/ad3927

This is a correction for 2024 Jpn. J. Appl. Phys. 63 04SP01

1347-4065/63/4/049401

Export citation and abstract BibTeX RIS

Due to an error in the production process, there are several corrections needed in this article.

In the caption of Fig. 10, ΔRS RS should be ΔRS. The correct caption and figure are shown below:

Fig. 10.

Fig. 10. Sheet resistance change ΔRS of LT-SWCNT-polyester fabrics under 100 bending cycles.

Standard image High-resolution image

On page 04SP01-5 the following sentence "Fig. 10 shows the ΔRS RS of the LT-SWCNT-polyester fabrics under 100 bending cycles. We observed about 1%–2% change in the ΔRS RS, which was considerably small." ΔRS RS should be corrected to ΔRS to read "Fig. 10 shows the ΔRS of the LT-SWCNT-polyester fabrics under 100 bending cycles. We observed about 1%–2% change in the ΔRS, which was considerably small."

On page 04SP01-6 the following sentence "Furthermore, we simulated the SE using HFSS for ΔRSRS of 1%–2% (Fig. S6), in which the SE of the LT-SWCNT-polyester fabrics was estimated to be almost unchanged after the 100 bending cycles." ΔRS RS should be corrected to ΔRS to read "Furthermore, we simulated the SE using HFSS for ΔRS of 1%–2% (Fig. S6), in which the SE of the LT-SWCNT-polyester fabrics was estimated to be almost unchanged after the 100 bending cycles."