Abstract
Extraction of cassiterite using alkaline decomposition of sodium carbonate (Na2CO3) has been studied. Cassiterite (SnO2) is a mineral ore that contains tin (Sn) about 57.82 wt% and impurities like quartz, ilmenite, monazite, rutile and zircon. The initial step for the process was to remove the impurities in cassiterite through washing and separation by a high magnetic separator (HTS). The aim of this research is to increase the added value of cassiterite from local area Indonesia that using alkaline decomposition to form sodium stannate (Na2SnO3). The result shows that cassiterite from Indonesia can form sodium stannate (Na2SnO3) which soluble with water in the leaching process. The longer the time for decomposition, the more phases of sodium stannate that will be formed. Optimum result reached when the decomposition process was done in 850 °C for 4 hours with a mole ratio Na2CO3 to cassiterite 3:2. High Score Plus (HSP) was used in this research to analyze the mass of sodium stannate (Na2SnO3). HSP analysis showed that mass of sodium stannate (Na2SnO3) is 70.3 wt%.
Export citation and abstract BibTeX RIS
Content from this work may be used under the terms of the Creative Commons Attribution 3.0 licence. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.