The main purpose of the work is to improve the magnetic and transport characteristics of 2G HTS tapes by creating an ordered array of artificial pinning centers. Using a picosecond laser exposure, a local modification of the HTS film were performed. The pulse energy varied from 300 to 4000 nJ, the pulse duration was 25 ps. A triangular array of micron size defects with a period of 50 μm was created. The dependences of the critical current and n-value change on the pulse energy were obtained. The parameters of the exposure resulting in an increase of the HTS tape critical current and tune of the I-V characteristic slope were found.

Export citation and abstract BibTeX RIS

Content from this work may be used under the terms of the Creative Commons Attribution 3.0 licence. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.

Please wait… references are loading.
10.1088/1742-6596/941/1/012078