Abstract
In this paper, an experimental study of laser dimensional processing of thermoset carbon fiber reinforced plastics with a thickness of 2 and 3 mm was performed. In the process of work test rig setup based on picosecond pulsed fiber laser with 1.06 microns wavelength and 30 W average power was developed. Experimental tests were carried out at the maximum average power, with laser beam moved by a galvanometric mirrors system. Cutting tests were executed with different scanning velocity, using different laser modes, number of repetitions, hatching distance and focal plane position without process gas. As a result of the research recommendations for the selection processing mode parameters, providing minimal heat affected zone, good kerf geometry and high cutting speed were produced.